MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MarkeTech Yttrium Vanadate (YVO4) Fiber Optic Crystal  (discontinued **)
Categories: Ceramic; Oxide

Material Notes: Large birefringence and wide transparency range (400 to 4000 nm); finds uses as fiber optic isolators, circulators, and beam displacers. Grown by Czochralski method.

Data provided by MarkeTech International. MarkeTech International is no longer in business.

Key Words: YVO4; Yttrium Vanadium Oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.22 g/cc0.152 lb/in³
a Lattice Constant 7.12 Å7.12 Å
c Lattice Constant 6.29 Å6.29 Å
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 5.05.0
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.43 µm/m-°C2.46 µin/in-°Fa direction
 11.37 µm/m-°C6.317 µin/in-°Fc direction
Thermal Conductivity 5.10 W/m-K35.4 BTU-in/hr-ft²-°Fc direction
 5.32 W/m-K36.9 BTU-in/hr-ft²-°Fa direction
Melting Point 1825 °C3317 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.951.95η o
 2.15542.1554η e
Transmission, Visible 90 %
@Wavelength >=400 nm
90 %
@Wavelength >=400 nm
transparent; thickness not reported
 
Descriptive Properties
Crystal StructureTetragonal

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SAES Getters Nd:YAG Solid State Laser Crystals (Nd-doped Y3Al5O12)
Borosilicate Glass
MarkeTech Beta Barium Borate (BBO) NLO Single Crystal
MarkeTech Rutile (TiO2) Fiber Optic Crystal
Nanocyl PREGCYL™ NC R2HM-01 Pre-impregnated UD/Fabric Carbon Fibers

C5MT830 / 120739

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.