MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Silicon Bronze, Copper Alloy, UNS C65680, M30 Temper, Rod
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: As Hot Extruded

Fabrication Properties: Good Suitability – Soldering, Brazing, Oxyacetylene Welding, Gas Shielded Arc Welding, Coated Metal Arc Welding, Spot Weld, Seam Weld, Butt Weld, Capacity for Being Cold Worked, Capacity for Being Hot Formed

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.302 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 125
@Load 3.00 kg
Tensile Strength 60.9 ksi
Tensile Strength, Yield 36.3 ksi0.2% Offset
Elongation at Break >= 10 %
Machinability 70 %
Forgeability 80 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000220 ohm-cm7.8% IACS
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 50.4 BTU-in/hr-ft²-°F
Melting Point 1652 - 1778 °F
Solidus 1652 °F
Liquidus 1778 °F
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.30 %
Copper, Cu >= 84 %
Iron, Fe <= 0.30 %
Lead, Pb <= 0.090 %
Manganese, Mn 0.010 - 0.090 %
Nickel, Ni <= 0.10 %
Phosphorus, P 0.050 - 0.15 %
Silicon, Si 2.5 - 4.5 %
Tin, Sn <= 0.30 %
Zinc, Zn 7.0 - 11 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC65680x3 / 292262

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.