MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Silicon Bronze, Copper Alloy, UNS C65680, M30 Temper, Rod
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: As Hot Extruded

Fabrication Properties: Good Suitability – Soldering, Brazing, Oxyacetylene Welding, Gas Shielded Arc Welding, Coated Metal Arc Welding, Spot Weld, Seam Weld, Butt Weld, Capacity for Being Cold Worked, Capacity for Being Hot Formed

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.36 g/cc0.302 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 125
@Load 3.00 kg
125
@Load 6.62 lb
Tensile Strength 420 MPa60900 psi
Tensile Strength, Yield 250 MPa36300 psi0.2% Offset
Elongation at Break >= 10 %>= 10 %
Machinability 70 %70 %
Forgeability 80 %80 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000220 ohm-cm0.0000220 ohm-cm7.8% IACS
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 7.26 W/m-K50.4 BTU-in/hr-ft²-°F
Melting Point 900.0 - 970.0 °C1652 - 1778 °F
Solidus 900.0 °C1652 °F
Liquidus 970.0 °C1778 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.30 %<= 0.30 %
Copper, Cu >= 84 %>= 84 %
Iron, Fe <= 0.30 %<= 0.30 %
Lead, Pb <= 0.090 %<= 0.090 %
Manganese, Mn 0.010 - 0.090 %0.010 - 0.090 %
Nickel, Ni <= 0.10 %<= 0.10 %
Phosphorus, P 0.050 - 0.15 %0.050 - 0.15 %
Silicon, Si 2.5 - 4.5 %2.5 - 4.5 %
Tin, Sn <= 0.30 %<= 0.30 %
Zinc, Zn 7.0 - 11 %7.0 - 11 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC65680x3 / 292262

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.