MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Evonik INFINAM® 9359 F PEEK
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: INFINAM® PEEK 9359F is a filament extruded from natural colored VESTAKEEP® polyether ether ketone (PEEK) resin. The semi-crystalline polymer features superior thermal and chemical resistance. Parts made from INFINAM® PEEK 9359F are of low flammability. Appropriate application fields include aerospace, automotive and other industries. Using INFINAM® PEEK 9359F with FDM technology will benefit our customers, for example less material consumption, superior mechanical properties of printed parts, and more freedom of design.
Industrial Sector: Automotive and Mobility, Aircraft and Aerospace, Energy, Oil and Gas, 3D Printing
Processing: 3D Printing
Delivery form: (Mono)filament
Resistance to: Heat (thermal stability), Fire / burn

Electrical: Insulating
Applications: Monofilament
Processing: Fused deposition molding, Additive manufacturing
Special Characteristics: Semi-crystalline, High heat resistant
Color: Natural color

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccISO 1183
Filament Diameter 1750 µm
Melt Flow 12.0 g/10 min
@Load 5.00 kg,
Temperature 380 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 70.0 MPaISO 527
Tensile Strength 90.0 MPaISO 527
Tensile Strength, Yield 90.0 MPaISO 527
Elongation at Break 5.00 %Nominal; ISO 527
Elongation at Yield 5.00 %ISO 527
Tensile Modulus 3600 MPaISO 527
Charpy Impact Unnotched NBon-edge Y, 3D printed parts; ISO 179/1eU
 NBupright Z, 3D printed parts; ISO 179/1eU
 NBISO 179/1eU
 NBISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²Type of failure: C; ISO 179/1eA
 7.00 kJ/m²Type of failure: C; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 340 °CISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 205 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 155 °CISO 75-1/-2
Glass Transition Temp, Tg 152 °CISO 11357-1/-2
Flammability, UL94 V-0
@Thickness 1.60 mm
IEC 60695-11-10
 
Processing PropertiesOriginal ValueComments
Drying Temperature <= 140 °C
Dry Time >= 4.00 hour
@Temperature 130 - 140 °C
Filament removed from spool
 >= 12.0 hour
@Temperature 100 - 120 °C
Filament on spool
 
Descriptive Properties
ColorNatural color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK7800 / 324932

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.