INFINAM® PEEK 9359F is a filament extruded from natural colored VESTAKEEP® polyether ether ketone (PEEK) resin. The semi-crystalline polymer features superior thermal and chemical resistance. Parts made from INFINAM® PEEK 9359F are of low flammability. Appropriate application fields include aerospace, automotive and other industries. Using INFINAM® PEEK 9359F with FDM technology will benefit our customers, for example less material consumption, superior mechanical properties of printed parts, and more freedom of design. Industrial Sector: Automotive and Mobility, Aircraft and Aerospace, Energy, Oil and Gas, 3D Printing Processing: 3D Printing Delivery form: (Mono)filament Resistance to: Heat (thermal stability), Fire / burnElectrical: Insulating Applications: Monofilament Processing: Fused deposition molding, Additive manufacturing Special Characteristics: Semi-crystalline, High heat resistant Color: Natural color Information provided by Evonik. |