MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kolon SPESIN® KP513UG PBT Alloy Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Extrusion Grade

Material Notes: Extrudable, delustering

Applications: Mono filament

Information provided by API-Kolon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/ccASTM D792
Moisture Absorption at Equilibrium 0.080 %60% RH; ASTM D570
Linear Mold Shrinkage 0.015 - 0.019 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 114ASTM D785
Tensile Strength 68.0 MPaASTM D638
Elongation at Break 40 %ASTM D638
Flexural Strength 79.0 MPaASTM D790
Flexural Modulus 196 MPaASTM D790
Izod Impact, Notched 49.0 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.7ASTM D150
Dielectric Strength 27.0 kV/mmASTM D149
Arc Resistance 110 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.0 µm/m-°CASTM D696
Melting Point 224 °CASTM D1525
Deflection Temperature at 0.46 MPa (66 psi) 150 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °CASTM D648
Flammability, UL94 HB

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem HB 0155 HDPE Blow Molding Polyethylene
Total Finathene® WR 201 B N HDPE blow molding
Total 51090 High Density Polyethylene - Blow Molding
Intercontinental Polymers HoPBT 310 HoPBT Polymer Type - Semi-Dull, Polyester Pellets
A. Schulman ComAlloy Comtuf® 420 Polyester - PBT, High Impact Modified

PKOKZ976 / 122678

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.