MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman ComAlloy Comtuf® 420 Polyester - PBT, High Impact Modified
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Impact Grade

Material Notes: Data provided by the manufacturer, ComAlloy International Company.

Superior toughness and impact resistance characterize Comtuf® materials

The ComAlloy product line has been integrated into the A Schulman product line.

Key Words: Polybutylene Terephthalate; ComAlloy International Company, subsidiary of A. Shulman Inc.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc0.0455 lb/in³
Linear Mold Shrinkage 0.018 cm/cm0.018 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 107107ASTM D785
Tensile Strength, Ultimate 28.0 MPa4060 psiASTM D638
Elongation at Break 34.2 %34.2 %ASTM D638
Flexural Strength 61.0 MPa8850 psiASTM D790
Flexural Modulus 1.70 GPa247 ksiASTM D790
Izod Impact, Notched 8.11 J/cm15.2 ft-lb/inASTM D256
Izod Impact, Unnotched NBNBASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 210 - 225 °C410 - 437 °F
Deflection Temperature at 0.46 MPa (66 psi) 154 °C309 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °C133 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Middle Barrel Temperature 224 - 241 °C435 - 466 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman COMTUF® 420 Impact Modified PBT
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
A. Schulman ComAlloy Comtuf® 461 Glass Reinforced, Impact Modified, PBT Alloy
Dow Elvaloy® PTW Ethylene/N-Butyl Acrylate/Glycidyl Methacrylate Copolymer
Eastman DuraStar MN610 Polymer, Natural

PASH31 / 24872

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.