MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
PCP-Canada ALCA MAX® 2XXX Cast Aluminum Mold Blocks/Plate
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes: ALCA MAX® is a 2xxx series mold blocks and plates ideal for large molds requiring extensive machining. It is characterized by an excellent dimensional stability, a high Brinell hardness and a good resistance to heat (less than 230°C). The low level of internal stress reduces considerably the deformation during and after machining. Typical applications include automotive, structural foam molds, rubber molds, investment cast, low-pressure injection molds, R.T.M. and R.I.M. molding. It provides strength, good hard anodizing response, weldability, and machinability (with sintered carbide materials).

Information provided by PCP-Canada.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.100 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 81
Tensile Strength, Ultimate 38000 psi
Tensile Strength, Yield 20000 psi
Elongation at Break 7 %in 2 inches
Modulus of Elasticity 10300 ksi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000044 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.4 µin/in-°F
@Temperature 20.0 - 100 °C
Thermal Conductivity 1128 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 230 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 92.38 - 94.56 %as remainder
Chromium, Cr 0.050 - 0.25 %
Copper, Cu 2.7 - 3.25 %
Iron, Fe 0.85 - 1.15 %
Magnesium, Mg 0.95 - 1.25 %
Manganese, Mn <= 0.070 %
Nickel, Ni 0.85 - 1.2 %
Silicon, Si <= 0.20 %
Titanium, Ti 0.040 - 0.10 %
Zinc, Zn <= 0.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 6063-T6
Aluminum 851.0-T5, Permanent Mold Cast
Aluminum 850.0-T5, Permanent Mold Cast
Aluminum 711.0-T1, Permanent Mold Cast
Alcoa QC-10® Aluminum Mold Alloy

NPCPC992 / 133290

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.