MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo MAGNUM™ 3416 SLG Acrylonitrile Butadiene Styrene (ABS) Resin  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Overview: The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines excellent processability with a stable light base color providing an ideal resin for self coloring. MAGNUM 3416 SLG is a new grade providing a unique property balance of ultra low gloss performance, excellent processing characteristics and high heat resistance.

Applications: Unpainted automotive interior trim components with enhanced requirements on strength, stiffness and low creep performance also at elevated temperatures.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccISO 1183
Apparent Bulk Density 0.650 g/ccISO 60
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 in/inISO 294-4
Melt Flow 8.5 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 39.0 MPaISO 527-2/50
Elongation at Break 60 %ISO 527-2/50
Tensile Modulus 1900 MPaInjection Molded; ISO 527-2
Flexural Strength 62.0 MPa3-point, 2 mm/min; ISO 178
Flexural Modulus 2050 MPa3-point, 2 mm/min; ISO 178
Charpy Impact, Notched 8.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 12.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °CUnannealed; ISO 75-2/A
Vicat Softening Point 107 °CISO 306/B50

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo Magnum™ 3416 SC Natural Plus ABS Resin
Envalior Akulon® K223-TP4 PA6-I, Dry, Impact Modified
Celanese Hostaform® C 9021 XAP Acetal Copolymer
Trinseo Magnum™ 347EZ ABS
Trinseo MAGNUM™ 3416NA ABS

PZZDWST077 / 142286

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.