MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo MAGNUM™ 3416NA ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: High heat, Low Gloss ABS resin with good practical toughness for injection molded automotive interior applications.

Applications: Door panels, Floor consoles, Instrument Panel & Sidewall trim parts.

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Apparent Bulk Density 0.660 g/cc0.0238 lb/in³ISO 60
Linear Mold Shrinkage, Flow 0.0055 - 0.0060 cm/cm0.0055 - 0.0060 in/inISO 294-4
Melt Flow  2.6 g/10 min
@Load 3.80 kg,
Temperature 230 °C
2.6 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ISO 1133
 8.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
8.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 43.0 MPa6240 psiISO 527-2/50
Elongation at Yield 3.0 %3.0 %ISO 527-2/50
Tensile Modulus 2.18 GPa316 ksiISO 527-2/1
Flexural Strength 66.0 MPa9570 psi2.0 mm/min, 3-points; ISO 178
Flexural Modulus 2.26 GPa328 ksi2.0 mm/min, 3-points; ISO 178
Izod Impact, Notched (ISO)  12.0 kJ/m²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
 20.0 kJ/m²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact, Notched  1.10 J/cm²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.80 J/cm²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °FUnannealed; ISO 75-2/A
Vicat Softening Point 107 °C225 °FISO 306/B50
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 302 °C576 °F
Middle Barrel Temperature 308 °C587 °F
Front Barrel Temperature 260 °C500 °F
Nozzle Temperature 254 °C489 °F
Melt Temperature 254 - 271 °C489 - 520 °F
Mold Temperature 38.0 - 60.0 °C100 - 140 °F
Drying Temperature 85.0 °C185 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
 
Descriptive Properties
Carbon Emission20 µg/gVDA 277
Fogging94 percent100°C, ISO 6452

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo Magnum™ FG960 ABS, High Impact
Trinseo Magnum™ 555 ABS
Trinseo MAGNUM™ 3904 Ultra Smooth ABS
Trinseo Magnum™ 3525 Acrylonitrile Butadiene Styrene (ABS)
Trinseo Magnum™ 3513 Acrylonitrile Butadiene Styrene (ABS)

PTRINS9072 / 197556

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.