MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo MAGNUM™ 3904 Ultra Smooth ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: MAGNUM™ 3904 Ultra Smooth is a high impact ABS resin for extrusion/thermoforming. This grade, is Trinseo’s lowest particulate (gels) content ABS grade, and is specially recommended for the most demanding surface finish applications.

Applications:

  • Automotive Interior
  • Furniture

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183/B
Apparent Bulk Density 0.650 g/cc0.0235 lb/in³ISO 60
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inISO 294-4
Melt Flow 4.7 g/10 min
@Load 10.0 kg,
Temperature 220 °C
4.7 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 37.0 MPa
@Thickness 4.00 mm
5370 psi
@Thickness 0.157 in
Injection Molded; ISO 527-2/50
Elongation at Yield 2.6 %
@Thickness 4.00 mm
2.6 %
@Thickness 0.157 in
Injection Molded; ISO 527-2/50
Tensile Modulus 1.82 GPa
@Thickness 4.00 mm
264 ksi
@Thickness 0.157 in
Injection Molded; ISO 527-2
Flexural Strength 58.0 MPa
@Thickness 4.00 mm
8410 psi
@Thickness 0.157 in
Injection Molded, 2.0 mm/min, 3-points; ISO 178
Flexural Modulus 1.90 GPa276 ksiInjection Molded, 2.0 mm/min, 3-points; ISO 178
Charpy Impact, Notched  1.80 J/cm²
@Temperature -30.0 °C
8.57 ft-lb/in²
@Temperature -22.0 °F
Injection Molded; ISO 179/1eA
 3.40 J/cm²
@Temperature 23.0 °C
16.2 ft-lb/in²
@Temperature 73.4 °F
Injection Molded; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 97.0 °C207 °FAnnealed; ISO 75-2/A
Vicat Softening Point 97.0 °C207 °FISO 306/B50
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo MAGNUM™ 3904 Acrylonitrile Butadiene Styrene (ABS) Resin
Trinseo MAGNUM™ 3904 Smooth Acrylonitrile Butadiene Styrene (ABS) Resin
Trinseo Magnum™ 3416 SC Natural Plus ABS Resin
Daicel CEVIAN® S5230 30% GF PC/ABS alloy
INEOS Styrolution Lustran® 248FC Acrylonitrile Butadiene Styrene (ABS)

PTRINS9064 / 197555

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.