MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

PlastiComp Complet® LCF40-PEEK Polyetheretherketone, 40% Long Carbon Fiber Reinforced  (discontinued **)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.

Polyetheretherketone with 40% long carbon fiber reinforcement

Information provided by PlastiComp, Inc.

Key Words: Complet® Long Fiber LCF
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Filler Content 40 %40 %Long Carbon Fiber
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 218 MPa31600 psiASTM D-638
Elongation at Break 0.70 %0.70 %ASTM D-638
Tensile Modulus 37.89 GPa5495 ksiASTM D-638
Flexural Strength 304 MPa44100 psiASTM D-790
Flexural Modulus 25.386 GPa3681.9 ksiASTM D-790
Izod Impact, Unnotched 7.26 J/cm13.6 ft-lb/inASTM D-4812

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled
Ovation Polymers Nemcon™ E PK DP104 Polyetheretherketone, Carbon Fiber Reinforced
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
RTP Company RTP 2285 LF TFE 15 Polyetheretherketone (PEEK), Carbon Fiber - PTFE Lubricated
Gharda Chemicals G-PAEK™ 1230CF Ultra High Performance PEK Polymer

PPLASTI946 / 171741

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.