MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Total PPC 4920WZ Polypropylene, Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: TOTAL Petrochemicals Polypropylene 4920WZ is a nucleated impact copolymer with a Melt Flow index of 105 g/10 min.

TOTAL Polypropylene 4920WZ is characterized by excellent stiffness and impact resistance, excellent antistatic properties, as well as extremely good flow properties to allow faster cycling through early demolding.

Total Polypropylene 4920WZcomplies with all applicable FDA regulations for food contact applications.

Total Polypropylene 4920WZ has been developed for high speed injection molding of thin-walled packaging containers and household articles.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.905 g/cc0.905 g/ccASTM D1505
Melt Flow 105 g/10 min105 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 25.0 MPa3630 psiASTM D638
Elongation at Yield 6.0 %6.0 %ASTM D638
Flexural Modulus 1.30 GPa189 ksiASTM D790
Izod Impact, Notched 0.500 J/cm0.937 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 160 - 165 °C320 - 329 °FTOTAL Method
Deflection Temperature at 0.46 MPa (66 psi) 110 °C230 °FPressure unspecified, Unannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Pro-fax PD702 Polypropylene Homopolymer, High Flow
PolyMirae Moplen 342R Injection Molding Grade Polypropylene
Aclo Accutech Polypropylene Copolymer CP0436G15M15CL Glass/Mineral Reinforced Coupled
A. Schulman TPP20AE63BK 20% Talc-Filled, Heat-Stabilized, Homopolymer Polypropylene containing 25% P.C.R.
A. Schulman PP 1247-01 Polypropylene Homopolymer Polypropylene

PTOTAL874 / 130599

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.