MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aclo Accutech Polypropylene Copolymer CP0436G15M15CL Glass/Mineral Reinforced Coupled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Glass/Mineral Reinforced

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ASTM D792
Linear Mold Shrinkage 0.0020 cm/cm0.0020 in/inMD; ASTM D955
Melt Flow 5.0 g/10 min5.0 g/10 minASTM D1238
Ash 30 %30 %ASTM D2584
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 5757ASTM D785
Tensile Strength at Break 33.0 MPa4790 psiASTM D638
Tensile Strength, Yield 35.0 MPa5080 psiASTM D638
Elongation at Break 9.0 %9.0 %ASTM D638
Elongation at Yield 4.0 %4.0 %ASTM D638
Tensile Modulus 3.050 GPa442.3 ksiASTM D638
Flexural Strength 53.0 MPa7690 psiASTM D790
Flexural Modulus 3.499 GPa507.5 ksiASTM D790
Izod Impact, Notched 1.17 J/cm2.20 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 151 °C304 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 112 °C234 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aclo Accutech Polypropylene Copolymer CP0436G20M10CL Glass/Mineral Reinforced Coupled
Aaron Industries AAROPRENE® TFIPP 2040 High Impact Talc Filled Polypropylene
Aaron Industries AAROPRENE® GFIPP 2040 High Impact Glass Filled Polypropylene
A. Schulman TPP20AE63BK 20% Talc-Filled, Heat-Stabilized, Homopolymer Polypropylene containing 25% P.C.R.
A. Schulman POLYFORT™ PP 1579 Impact Grade Polypropylene

PACLO165 / 22420

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.