MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Parker Chomerics CHO-JAC® CJ-021 Flat Cable EMI Shield
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: Description: CHO-JAC shielding is a high quality flat cable jacket designed to attenuate RF signals and bring digital electronic devices into EMC compliance at an attractive cost. It is lightweight and very flexible, easing cable routing during assembly. The jacket is designed with a 360° aluminum or copper shield, bonded with a metal overlap to a polyester layer which resists scuff, wear and tear. Metal-to-metal contact is established as the jacket wrap is completed. This design provides the maximum EMI shielding when properly sealed and terminated. Integral wires simplify folding and termination, and provide crack resistance. Pressure-sensitive adhesive eliminates heat-sealing irons and zippers.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Electrical PropertiesMetricEnglishComments
Shielding Effectiveness  -10.0 dB
@Frequency 1.30e+8 Hz
-10.0 dB
@Frequency 1.30e+8 Hz
Jacketing terminated with wires only
 -10.0 dB
@Frequency 6.00e+8 Hz
-10.0 dB
@Frequency 6.00e+8 Hz
Jacketing terminated with wires only
 -7.00 dB
@Frequency 2.70e+8 Hz
-7.00 dB
@Frequency 2.70e+8 Hz
Jacketing terminated with wires only
 -5.00 dB
@Frequency 2.00e+8 Hz
-5.00 dB
@Frequency 2.00e+8 Hz
Jacketing terminated with wires only
 5.0 dB
@Frequency 4.00e+8 Hz
5.0 dB
@Frequency 4.00e+8 Hz
Jacketing terminated with wires only
 15 dB
@Frequency 8.50e+8 Hz
15 dB
@Frequency 8.50e+8 Hz
Jacketing terminated with wires only
 19 dB
@Frequency 6e+7 Hz
19 dB
@Frequency 6e+7 Hz
Jacketing terminated with wires only
 40 dB
@Frequency 1e+9 Hz
40 dB
@Frequency 1e+9 Hz
360° Ground Termination
 49 dB
@Frequency 4.00e+8 Hz
49 dB
@Frequency 4.00e+8 Hz
360° Ground Termination
 53 dB
@Frequency 4.00e+7 Hz
53 dB
@Frequency 4.00e+7 Hz
360° Ground Termination
 53 dB
@Frequency 1e+8 Hz
53 dB
@Frequency 1e+8 Hz
360° Ground Termination

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyester Thermoplastic Elastomer
Overview of materials for Polyester Film
Dielectric Polymers NT-5521-2 Photo Processing Tape
C.O.I.M. DIEXTER® G214 Polyol Polyester
C.O.I.M. DIEXTER® G120 Polyol Polyester

PCHOME429 / 131139

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.