MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polyester Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.00 - 1.36 g/cc0.0361 - 0.0491 lb/in³Average value: 1.19 g/cc Grade Count:148
Water Absorption 0.100 - 0.800 %0.100 - 0.800 %Average value: 0.500 % Grade Count:42
Moisture Absorption at Equilibrium 0.200 - 0.560 %0.200 - 0.560 %Average value: 0.388 % Grade Count:31
Water Absorption at Saturation 0.500 - 0.900 %0.500 - 0.900 %Average value: 0.660 % Grade Count:5
Viscosity 400 - 461000 cP400 - 461000 cPAverage value: 204000 cP Grade Count:4
 200 - 85000 cP
@Temperature 160 - 232 °C
200 - 85000 cP
@Temperature 320 - 450 °F
Average value: 43100 cP Grade Count:5
Viscosity Test 68.0 - 150 cm³/g0.680 - 1.50 dl/gAverage value: 109 cm³/g Grade Count:3
Molecular Weight 458 g/mol458 g/molAverage value: 458 g/mol Grade Count:21
Maximum Moisture Content 0.0100 - 0.05000.0100 - 0.0500Average value: 0.0214 Grade Count:51
Linear Mold Shrinkage 0.00400 - 0.0220 cm/cm0.00400 - 0.0220 in/inAverage value: 0.0123 cm/cm Grade Count:75
Linear Mold Shrinkage, Transverse 0.0100 - 0.0220 cm/cm0.0100 - 0.0220 in/inAverage value: 0.0176 cm/cm Grade Count:11
Melt Flow 0.500 - 300 g/10 min0.500 - 300 g/10 minAverage value: 21.8 g/10 min Grade Count:126
 
Chemical PropertiesMetricEnglishComments
Acid Value 2.00 - 3.002.00 - 3.00Average value: 2.83 Grade Count:6
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 65.0 - 99.065.0 - 99.0Average value: 90.2 Grade Count:55
Hardness, Shore D 19.0 - 78.019.0 - 78.0Average value: 48.9 Grade Count:123
Tensile Strength, Ultimate 2.00 - 56.5 MPa290 - 8200 psiAverage value: 28.5 MPa Grade Count:116
Tensile Strength, Yield 2.00 - 72.2 MPa290 - 10500 psiAverage value: 32.9 MPa Grade Count:40
Elongation at Break 8.00 - 2000 %8.00 - 2000 %Average value: 496 % Grade Count:142
Elongation at Yield 6.00 - 44.0 %6.00 - 44.0 %Average value: 22.1 % Grade Count:8
Modulus of Elasticity 0.0130 - 2.25 GPa1.89 - 326 ksiAverage value: 0.345 GPa Grade Count:37
 0.0466692 - 3.14966 GPa
@Temperature -100 - 110 °C
6.76890 - 456.827 ksi
@Temperature -148 - 230 °F
Average value: 1.26 GPa Grade Count:2
Flexural Yield Strength 1.00 - 89.6 MPa145 - 13000 psiAverage value: 20.0 MPa Grade Count:28
Flexural Modulus 0.0130 - 2.76 GPa1.89 - 400 ksiAverage value: 0.369 GPa Grade Count:116
 0.00800 - 2.50 GPa
@Temperature -40.0 - 100 °C
1.16 - 363 ksi
@Temperature -40.0 - 212 °F
Average value: 0.758 GPa Grade Count:10
Compressive Modulus 0.00240 - 0.0392 GPa0.348 - 5.69 ksiAverage value: 0.0153 GPa Grade Count:29
Resilience 40.0 - 81.040.0 - 81.0Average value: 61.4 Grade Count:36
Flex Crack Resistance 1.00e+61.00e+6Average value: 1.00e+6 Grade Count:7
Izod Impact, Notched 0.374 J/cm - NB0.700 ft-lb/in - NBAverage value: 4.24 J/cm Grade Count:75
 0.26695 J/cm - NB
@Temperature -40.0 - -40.0 °C
0.50011 ft-lb/in - NB
@Temperature -40.0 - -40.0 °F
Average value: 1.10 J/cm Grade Count:8
 0.294199 - 980.567 J/cm
@Temperature -40.0 - -40.0 °C
0.551156 - 1837.00 ft-lb/in
@Temperature -40.0 - -40.0 °F
Average value: 1.10 J/cm Grade Count:29
 0.294199 - 980.567 J/cm
@Thickness 6.40 - 6.40 mm
0.551156 - 1837.00 ft-lb/in
@Thickness 0.252 - 0.252 in
Average value: 1.10 J/cm Grade Count:29
Izod Impact, Unnotched 13.3 - 5340 J/cm25.0 - 10000 ft-lb/inAverage value: 14.7 J/cm Grade Count:5
Izod Impact, Notched (ISO) 4.70 - 21000 kJ/m²2.24 - 9990 ft-lb/in²Average value: 20.9 kJ/m² Grade Count:16
 3.50 - 20997.9 kJ/m²
@Temperature -40.0 - -20.0 °C
1.67 - 9991.75 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 19.9 kJ/m² Grade Count:18
Charpy Impact Unnotched 7.10 J/cm² - NB33.8 ft-lb/in² - NBAverage value: 8.65 J/cm² Grade Count:26
 0.450 J/cm² - NB
@Temperature -40.0 - -30.0 °C
2.14 ft-lb/in² - NB
@Temperature -40.0 - -22.0 °F
Average value: 0.450 J/cm² Grade Count:20
Charpy Impact, Notched 0.940 J/cm² - NB4.47 ft-lb/in² - NBAverage value: 4.98 J/cm² Grade Count:38
 0.450 J/cm² - NB
@Temperature -40.0 - -30.0 °C
2.14 ft-lb/in² - NB
@Temperature -40.0 - -22.0 °F
Average value: 5.20 J/cm² Grade Count:28
Gardner Impact >= 32.7657 J
@Temperature -40.0 - -40.0 °C
>= 24.1667 ft-lb
@Temperature -40.0 - -40.0 °F
Average value: 49.4 J Grade Count:2
Tensile Creep Modulus, 1 hour  30.7907 - 111.849 MPa
@Temperature 40.0 - 100 °C
4465.82 - 16222.4 psi
@Temperature 104 - 212 °F
Average value: 66.3 MPa Grade Count:2
 30.7907 - 111.849 MPa
@Pressure 0.500 - 7.00 MPa
4465.82 - 16222.4 psi
@Pressure 72.5 - 1020 psi
Average value: 66.3 MPa Grade Count:2
Tensile Creep Modulus, 1000 hours  21.7457 - 83.3376 MPa
@Temperature 40.0 - 100 °C
3153.95 - 12087.1 psi
@Temperature 104 - 212 °F
Average value: 49.2 MPa Grade Count:2
 21.7457 - 83.3376 MPa
@Pressure 0.500 - 7.00 MPa
3153.95 - 12087.1 psi
@Pressure 72.5 - 1020 psi
Average value: 49.2 MPa Grade Count:2
Tear Strength 40.0 - 362 kN/m228 - 2070 pliAverage value: 149 kN/m Grade Count:83
Taber Abrasion, mg/1000 Cycles 5.00 - 90.05.00 - 90.0Average value: 20.7 Grade Count:33
Compression Set 1.00 - 65.0 %1.00 - 65.0 %Average value: 42.9 % Grade Count:37
Torsional Stiffness 20.0 - 500 MPa2900 - 72500 psiAverage value: 198 MPa Grade Count:11
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+11 - 4.00e+16 ohm-cm1.00e+11 - 4.00e+16 ohm-cmAverage value: 1.21e+15 ohm-cm Grade Count:59
Surface Resistance 1.00e+12 - 2.00e+17 ohm1.00e+12 - 2.00e+17 ohmAverage value: 2.66e+16 ohm Grade Count:16
Dielectric Constant 3.30 - 5.103.30 - 5.10Average value: 4.47 Grade Count:12
Dielectric Strength 11.8 - 75.0 kV/mm300 - 1910 kV/inAverage value: 23.1 kV/mm Grade Count:59
Dissipation Factor 0.0200 - 0.04000.0200 - 0.0400Average value: 0.0336 Grade Count:11
Arc Resistance 120 - 240 sec120 - 240 secAverage value: 165 sec Grade Count:4
Comparative Tracking Index 100 - 600 V100 - 600 VAverage value: 590 V Grade Count:40
Hot Wire Ignition, HWI 15.0 - 120 sec15.0 - 120 secAverage value: 47.8 sec Grade Count:4
High Amp Arc Ignition, HAI 120 arcs120 arcsAverage value: 120 arcs Grade Count:4
 
Thermal PropertiesMetricEnglishComments
CTE, linear 23.4 - 250 µm/m-°C13.0 - 139 µin/in-°FAverage value: 169 µm/m-°C Grade Count:45
CTE, linear, Transverse to Flow 170 - 190 µm/m-°C94.4 - 106 µin/in-°FAverage value: 183 µm/m-°C Grade Count:3
Melting Point 83.0 - 223 °C181 - 433 °FAverage value: 194 °C Grade Count:121
Maximum Service Temperature, Air 68.0 - 161 °C154 - 322 °FAverage value: 113 °C Grade Count:19
Deflection Temperature at 0.46 MPa (66 psi) 42.0 - 145 °C108 - 293 °FAverage value: 84.4 °C Grade Count:37
Deflection Temperature at 1.8 MPa (264 psi) 45.0 - 130 °C113 - 266 °FAverage value: 62.9 °C Grade Count:13
Vicat Softening Point 42.0 - 210 °C108 - 410 °FAverage value: 151 °C Grade Count:62
Softening Point 92.0 - 166 °C198 - 331 °FAverage value: 131 °C Grade Count:5
Brittleness Temperature -78.0 - -50.0 °C-108 - -58.0 °FAverage value: -64.3 °C Grade Count:32
Glass Transition Temp, Tg -65.0 - 5.50 °C-85.0 - 41.9 °FAverage value: -30.8 °C Grade Count:7
UL RTI, Electrical 50.0 °C122 °FAverage value: 50.0 °C Grade Count:6
UL RTI, Mechanical with Impact 50.0 °C122 °FAverage value: 50.0 °C Grade Count:6
UL RTI, Mechanical without Impact 50.0 °C122 °FAverage value: 50.0 °C Grade Count:6
Flammability, UL94 HB - V-0HB - V-0Grade Count:56
Oxygen Index 20.0 - 37.2 %20.0 - 37.2 %Average value: 29.8 % Grade Count:3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 300 °C68.0 - 572 °FAverage value: 137 °C Grade Count:23
Nozzle Temperature 170 - 271 °C338 - 520 °FAverage value: 222 °C Grade Count:38
Adapter Temperature 180 - 260 °C356 - 500 °FAverage value: 224 °C Grade Count:27
Die Temperature 170 - 260 °C338 - 500 °FAverage value: 220 °C Grade Count:37
Melt Temperature 150 - 290 °C302 - 554 °FAverage value: 215 °C Grade Count:66
Mold Temperature 10.0 - 93.3 °C50.0 - 200 °FAverage value: 38.8 °C Grade Count:53
Drying Temperature 80.0 - 127 °C176 - 260 °FAverage value: 93.1 °C Grade Count:68
Moisture Content 0.0100 - 0.150 %0.0100 - 0.150 %Average value: 0.0492 % Grade Count:13
Injection Pressure 4.96 - 103 MPa720 - 15000 psiAverage value: 59.2 MPa Grade Count:5
Cure Time 0.0333 - 0.250 min0.000556 - 0.00417 hourAverage value: 0.118 min Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber
Overview of materials for Polyether Ester Elastomer
Overview of materials for Styrenic Elastomer (TES)

O5410 / 78499

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.