MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Stratasys® ABSi
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; ABS Polymer

Material Notes: ABSi™ is an ideal material for conceptual modeling, functional prototyping and direct digital manufacturing. Its strength is superior to standard ABS, and the translucent nature of ABSi is beneficial for monitoring material flow and light transmission, most commonly used for medical and automotive applications. When combined with a Fortus® 3D Printer, ABSi yields parts that are visually unique, dimensionally accurate, durable and hold their shape over time.

Information provided by Stratasys®

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 108108ASTM D785
Tensile Strength 37.0 MPa
@Thickness 3.17 mm
5370 psi
@Thickness 0.125 in
Type 1, 0.2”/min; ASTM D638
Tensile Modulus 1.92 GPa
@Thickness 3.17 mm
278 ksi
@Thickness 0.125 in
Type 1, 0.2”/min; ASTM D638
Flexural Strength 62.0 MPa8990 psiMethod 1, 0.05”/min; ASTM D790
Flexural Modulus 1.92 GPa278 ksiMethod 1, 0.05”/min; ASTM D790
Izod Impact, Notched 0.964 J/cm1.81 ft-lb/inMethod A; ASTM D256
Izod Impact, Unnotched 1.911 J/cm3.580 ft-lb/inMethod A; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.50e+9 - 6.10e+10 ohm-cm1.50e+9 - 6.10e+10 ohm-cmASTM D257
Dielectric Constant 3.4 - 3.63.4 - 3.6ASTM D150-98
Dielectric Strength 3.94 - 12.6 kV/mm100 - 320 kV/inASTM D149-09, Method A
Dissipation Factor 0.12 - 0.150.12 - 0.15ASTM D150-98
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.1 µm/m-°C6.72 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 86.0 °C
@Thickness 3.17 mm
187 °F
@Thickness 0.125 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 73.0 °C
@Thickness 3.17 mm
163 °F
@Thickness 0.125 in
unannealed; ASTM D648
Glass Transition Temp, Tg 116 °C241 °FDMA (SSYS)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Stratasys® ABS-M30
Stratasys® Ultem 9085 for Rapid Prototyping
Stratasys® PC-ABS
Stratasys® ABS-M30i
Stratasys® PPSF Polyphenylsulfone for 3D Printing

PSTRAT003 / 78545

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.