MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Stratasys® PC-ABS
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: PC-ABS is a blend of polycarbonate (PC) and acrylonitrile butadiene styrene (ABS) thermoplastics. The result is an FDM filament that exhibits optimal characteristics of each – excellent strength, high toughness and heat resistance, and good flexural strength. PC-ABS exhibits the strength of PC but the impact resistance of ABS. PC-ABS is suitable for a variety of applications that include prototyping, tooling and low-volume production. Available colors are black and white.

Information provided by Stratasys®

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccXY, XZ/ZX Orientations; ASTM D257
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 25.0 MPa3630 psiZX Orientation; ASTM D638
 34.0 MPa4930 psiXZ Orientation; ASTM D638
Tensile Strength, Yield 36.0 MPa5220 psiXZ Orientation; ASTM D638
Elongation at Break 1.8 %1.8 %ZX Orientation; ASTM D638
 4.7 %4.7 %XZ Orientation; ASTM D638
Elongation at Yield 3.01 %3.01 %XZ Orientation; ASTM D638
Modulus of Elasticity 1.80 GPa261 ksiZX Orientation; ASTM D638
 1.98 GPa287 ksiXZ Orientation; ASTM D638
Flexural Strength 45.0 MPa6530 psiZX Orientation; ASTM D790, Procedure A
Flexural Modulus 1.68 GPa244 ksiZX Orientation; ASTM D790, Procedure A
 1.90 GPa276 ksiXZ Orientation; ASTM D790, Procedure A
Flexural Strain at Break 3.5 %3.5 %ZX Orientation; ASTM D790, Procedure A
Compressive Yield Strength 95.0 MPa13800 psiXZ Orientation; ASTM D695
 170 MPa24700 psiZX Orientation; ASTM D695
Compressive Modulus 1.95 GPa283 ksiXZ Orientation; ASTM D695
 2.11 GPa306 ksiZX Orientation; ASTM D695
Izod Impact, Notched 0.350 J/cm0.656 ft-lb/inZX Orientation; ASTM D256, ASTM D4812
 2.40 J/cm4.50 ft-lb/inXZ Orientation; ASTM D256, ASTM D4812
Izod Impact, Unnotched 1.00 J/cm1.87 ft-lb/inZX Orientation; ASTM D256, ASTM D4812
 6.55 J/cm12.3 ft-lb/inXZ Orientation; ASTM D256, ASTM D4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 6.80e+14 ohm-cm6.80e+14 ohm-cmXY, XZ/ZX Orientations; ASTM D257
Dielectric Constant  2.62
@Frequency 1000 Hz
2.62
@Frequency 1000 Hz
XY Orientation; ASTM D150
 2.74
@Frequency 2.00e+6 Hz
2.74
@Frequency 2.00e+6 Hz
XY Orientation; ASTM D150
 2.74
@Frequency 1000 Hz
2.74
@Frequency 1000 Hz
XZ/ZX Orientation; ASTM D150
 2.88
@Frequency 2.00e+6 Hz
2.88
@Frequency 2.00e+6 Hz
XZ/ZX Orientation; ASTM D150
Dissipation Factor  0.0010
@Frequency 1000 Hz
0.0010
@Frequency 1000 Hz
XY Orientation; ASTM D150
 0.0010
@Frequency 2.00e+6 Hz
0.0010
@Frequency 2.00e+6 Hz
XZ/ZX Orientation; ASTM D150
 0.0020
@Frequency 2.00e+6 Hz
0.0020
@Frequency 2.00e+6 Hz
XY Orientation; ASTM D150
 0.0020
@Frequency 1000 Hz
0.0020
@Frequency 1000 Hz
XZ/ZX Orientation; ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear  -60.0 µm/m-°C
@Temperature 50.0 - 90.0 °C
-33.3 µin/in-°F
@Temperature 122 - 194 °F
XY Orientation; ASTM E831
 0.500 µm/m-°C
@Temperature 35.0 - 50.0 °C
0.278 µin/in-°F
@Temperature 95.0 - 122 °F
XY Orientation; ASTM E831
 35.0 µm/m-°C
@Temperature -50.0 - 35.0 °C
19.4 µin/in-°F
@Temperature -58.0 - 95.0 °F
XY Orientation; ASTM E831
 70.0 µm/m-°C
@Temperature -50.0 - 95.0 °C
38.9 µin/in-°F
@Temperature -58.0 - 203 °F
XZ/ZX Orientation; ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 125 °C257 °FXY, XZ/ZX Orientations; ASTM D648 Method B
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FXY, XZ/ZX Orientations; ASTM D648 Method B
Glass Transition Temp, Tg 105 °C221 °FInflection Point, XY, XZ/ZX; ASTM D7426

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Stratasys® Ultem 9085 for Rapid Prototyping
Stratasys® PC Polycarbonate for 3D Printing
Stratasys® ABS-M30
Stratasys® ABSi
Stratasys® ABS-M30i

PSTRAT006 / 78548

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.