MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Stratasys® PC Polycarbonate for 3D Printing
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: PC is a polycarbonate FDM® filament that brings the attributes of this industrial plastic to 3D printing applications. PC is characterized by its high strength and impact resistance, coupled with dimensional stability and heat resistance. These attributes make it a good choice for 3D printed prototypes, parts and tools that demand higher material properties than ABS or ASA. FDM PC is available in white and is compatible with both breakaway and soluble support materials.PC runs the Xtend 500 Fortus Plus option, which enables more than 400 hours of unattended build time.

Information provided by Stratasys®

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccXY, XZ/ZX Orientations; ASTM D257
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 35.0 MPa5080 psiZX Orientation; ASTM D638
 57.0 MPa8270 psiXZ Orientation; ASTM D638
Tensile Strength, Yield 60.0 MPa8700 psiXZ Orientation; ASTM D638
Elongation at Break 1.8 %1.8 %ZX Orientation; ASTM D638
 5.2 %5.2 %XZ Orientation; ASTM D638
Elongation at Yield 4.9 %4.9 %XZ Orientation; ASTM D638
Modulus of Elasticity 2.10 GPa305 ksiZX Orientation; ASTM D638
 2.25 GPa326 ksiXZ Orientation; ASTM D638
Flexural Strength 75.0 MPa10900 psiZX Orientation; ASTM D790, Procedure A
 90.0 MPa
@Strain 5.0 %
13100 psi
@Strain 5.0 %
ZX Orientation; ASTM D790, Procedure A
Flexural Modulus 1.88 GPa273 ksiZX Orientation; ASTM D790, Procedure A
 2.15 GPa312 ksiXZ Orientation; ASTM D790, Procedure A
Flexural Strain at Break 4.5 %4.5 %ZX Orientation; ASTM D790, Procedure A
Compressive Yield Strength 245 MPa35500 psiXZ Orientation; ASTM D695
 290 MPa42100 psiZX Orientation; ASTM D695
Compressive Modulus 1.95 GPa283 ksiXZ Orientation; ASTM D695
 2.11 GPa306 ksiZX Orientation; ASTM D695
Izod Impact, Notched 0.250 J/cm0.468 ft-lb/inZX Orientation; ASTM D256, ASTM D4812
 0.750 J/cm1.41 ft-lb/inXZ Orientation; ASTM D256, ASTM D4812
Izod Impact, Unnotched 2.30 J/cm4.31 ft-lb/inZX Orientation; ASTM D256, ASTM D4812
 7.60 J/cm14.2 ft-lb/inXZ Orientation; ASTM D256, ASTM D4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.80e+14 ohm-cm3.80e+14 ohm-cmXY, XZ/ZX Orientations; ASTM D257
Dielectric Constant  2.53
@Frequency 2.00e+6 Hz
2.53
@Frequency 2.00e+6 Hz
XY Orientation; ASTM D150
 2.66
@Frequency 1000 Hz
2.66
@Frequency 1000 Hz
XY Orientation; ASTM D150
 2.69
@Frequency 2.00e+6 Hz
2.69
@Frequency 2.00e+6 Hz
XZ/ZX Orientation; ASTM D150
 2.84
@Frequency 1000 Hz
2.84
@Frequency 1000 Hz
XZ/ZX Orientation; ASTM D150
Dissipation Factor  0.0020
@Frequency 1000 Hz
0.0020
@Frequency 1000 Hz
XY Orientation; ASTM D150
 0.0030
@Frequency 2.00e+6 Hz
0.0030
@Frequency 2.00e+6 Hz
XY Orientation; ASTM D150
 0.0080
@Frequency 2.00e+6 Hz
0.0080
@Frequency 2.00e+6 Hz
XY, XZ/ZX Orientations; ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.0 µm/m-°C
@Temperature 75.0 - 130 °C
5.56 µin/in-°F
@Temperature 167 - 266 °F
XY Orientation; ASTM E831
 35.0 µm/m-°C
@Temperature 30.0 - 75.0 °C
19.4 µin/in-°F
@Temperature 86.0 - 167 °F
XY Orientation; ASTM E831
 50.0 µm/m-°C
@Temperature -50.0 - 30.0 °C
27.8 µin/in-°F
@Temperature -58.0 - 86.0 °F
XY Orientation; ASTM E831
 50.0 µm/m-°C
@Temperature -50.0 - 120 °C
27.8 µin/in-°F
@Temperature -58.0 - 248 °F
XZ/ZX Orientation; ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 145 °C293 °FXY, XZ/ZX Orientations; ASTM D648 Method B
Deflection Temperature at 1.8 MPa (264 psi) 140 °C284 °FXY, XZ/ZX Orientations; ASTM D648 Method B
Glass Transition Temp, Tg 140 °C284 °FInflection Point, XY, XZ/ZX; ASTM D7426

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Stratasys® Ultem 9085 for Rapid Prototyping
Stratasys® PC-ABS
Stratasys® ABSi
Stratasys® ABS-M30
Stratasys® ABS-M30i

PSTRAT005 / 78547

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.