MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Saint-Gobain CHR® 6004 Glass-Foil Backing Silicone Adhesive Pressure Sensitive Tape
Categories: Polymer; Adhesive; Tape; Thermoset; Silicone

Material Notes: CHR® 06004 is manufactured from a laminate of aluminium foil and silicone adhesive impregnated fibreglass cloth.

Features/Benefits: CHR® 06004 offers excellent abrasion resistance and is very conformable. The specially formulated silicone adhesive system provides an excellent bond to the part being masked and holds the tape firmly in place throughout the entire spraying process. It also removes cleanly reducing cleaning of the part.

Applications: Saint-Gobain Performance Plastics 06004 is used in applications where high temperatures and/or abrasion are issues. CHR® 06004 is used to mask parts during thermal spray applications, and because of the abrasion resistance of the aluminium foil, is effective when used in the HVOF process.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tear Strength 27.2 kN/m155 pliTensile Strength
Peel Strength 0.660 kN/m3.77 pliAdhesion to Steel
 0.660 kN/m3.77 pliAdhesion to Aluminum
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -73.0 °C-99.4 °F
 
Descriptive Properties
ColorAluminum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
6004 Aluminum Composition Spec

PSTGQZ384 / 68898

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.