MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Abatron AboCast/AboCure 8109-2
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: High melting point. Filled version.

Processing: 100/10 pbw; 90 minute potlife; mix at 130-140°C (270 °F); cures in 16 h/120°C (250°F), 10 h/140°C (285°F), 8 h/160°C (320°F), 2 h/ 200°C (390°F).

Applications: Heavy duty casting and potting.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.75 g/cc
Water Absorption 0.25 - 0.30 %(60x10X4 mm bar) after 10 days at 20°C (77°F)
 0.30 - 0.35 %(60x10X4 mm bar) after 1 hour at 100°C (212°F)
Viscosity 5000 - 50000 cP
@Temperature 120 °C
Vapor Pressure <= 0.0100 torr
@Temperature 20.0 °C
AboCure
 <= 1.00 torr
@Temperature 180 °C
AboCast
 1.00 torr
@Temperature 100 °C
AboCure
 2.80 torr
@Temperature 120 °C
AboCure
 10.0 torr
@Temperature 135 °C
AboCure
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 62.05 MPa
Flexural Yield Strength 131 MPa
Compressive Yield Strength 193.1 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.50e+16 ohm-cm
Dielectric Constant 3.7 - 4.0
@Frequency 50 Hz
 3.9 - 4.2
@Frequency 1000 Hz
 4.0 - 4.2
@Frequency 1e+6 Hz
Dielectric Strength 17.72 - 20.67 kV/mm
@Thickness 3.17 mm
Short time value
Dissipation Factor 0.0090 - 0.014
@Frequency 50 Hz
 0.0090 - 0.015
@Frequency 1000 Hz
 0.015 - 0.025
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 30.0 - 35.0 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 0.590 - 0.670 W/m-K
Maximum Service Temperature, Air 115 °CDeflection temperature; load unknown
 
Processing PropertiesOriginal ValueComments
Processing Temperature 130 - 140 °C
Pot Life 90.0 min
@Temperature 120 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Parker Chomerics CHO-BOND® 1075 Silicone RTV Adhesive/Sealant
Overview of materials for Epoxy, Thermally Conductive
Overview of materials for Epoxy Molding Compound
Henkel Loctite® Output™ 315 Acrylic Adhesive
Epoxyset Epoxibond EB-309 Low Expansion Epoxy Adhesive

PABEQ1 / 22016

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.