MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Abatron AboCast/AboCure 8109-2
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: High melting point. Filled version.

Processing: 100/10 pbw; 90 minute potlife; mix at 130-140°C (270 °F); cures in 16 h/120°C (250°F), 10 h/140°C (285°F), 8 h/160°C (320°F), 2 h/ 200°C (390°F).

Applications: Heavy duty casting and potting.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.75 g/cc0.0632 lb/in³
Water Absorption 0.25 - 0.30 %0.25 - 0.30 %(60x10X4 mm bar) after 10 days at 20°C (77°F)
 0.30 - 0.35 %0.30 - 0.35 %(60x10X4 mm bar) after 1 hour at 100°C (212°F)
Viscosity 5000 - 50000 cP
@Temperature 120 °C
5000 - 50000 cP
@Temperature 248 °F
Vapor Pressure  <= 0.0000133 bar
@Temperature 20.0 °C
<= 0.0100 torr
@Temperature 68.0 °F
AboCure
 <= 0.00133 bar
@Temperature 180 °C
<= 1.00 torr
@Temperature 356 °F
AboCast
 0.00133 bar
@Temperature 100 °C
1.00 torr
@Temperature 212 °F
AboCure
 0.00373 bar
@Temperature 120 °C
2.80 torr
@Temperature 248 °F
AboCure
 0.0133 bar
@Temperature 135 °C
10.0 torr
@Temperature 275 °F
AboCure
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 62.05 MPa9000 psi
Flexural Yield Strength 131 MPa19000 psi
Compressive Yield Strength 193.1 MPa28010 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.50e+16 ohm-cm>= 1.50e+16 ohm-cm
Dielectric Constant  3.7 - 4.0
@Frequency 50 Hz
3.7 - 4.0
@Frequency 50 Hz
 3.9 - 4.2
@Frequency 1000 Hz
3.9 - 4.2
@Frequency 1000 Hz
 4.0 - 4.2
@Frequency 1e+6 Hz
4.0 - 4.2
@Frequency 1e+6 Hz
Dielectric Strength 17.72 - 20.67 kV/mm
@Thickness 3.17 mm
450.1 - 525.0 kV/in
@Thickness 0.125 in
Short time value
Dissipation Factor  0.0090 - 0.014
@Frequency 50 Hz
0.0090 - 0.014
@Frequency 50 Hz
 0.0090 - 0.015
@Frequency 1000 Hz
0.0090 - 0.015
@Frequency 1000 Hz
 0.015 - 0.025
@Frequency 1e+6 Hz
0.015 - 0.025
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.0 - 35.0 µm/m-°C
@Temperature 20.0 °C
16.7 - 19.4 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.590 - 0.670 W/m-K4.09 - 4.65 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 115 °C239 °FDeflection temperature; load unknown
 
Processing PropertiesMetricEnglishComments
Processing Temperature 130 - 140 °C266 - 284 °F
Pot Life 90.0 min
@Temperature 120 °C
90.0 min
@Temperature 248 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics CHO-BOND® 1075 Silicone RTV Adhesive/Sealant
Overview of materials for Epoxy, Thermally Conductive
Overview of materials for Epoxy Molding Compound
Henkel Loctite® Output™ 315 Acrylic Adhesive
Epoxyset Epoxibond EB-309 Low Expansion Epoxy Adhesive

PABEQ1 / 22016

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.