MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hostalen GD 7255 LS High Density Polyethylene (HDPE), Injection Molded
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Hostalen GD 7255 LS is a high density polyethylene resin stabilized to prevent UV degradation. It's used in general injection molding applications such as pallets and dust bin bodies. Hostalen GD 7255 LS is available in pellet form, and exhibits high ESCR, good impact resistance, flowability and low warpage. Hostalen GD 7255 LS is not intended for use in medical and pharmaceutical applications. Applications: Crates, House wares, Industrial, Panels & Profiles, Sports, Leisure & Toys

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.955 g/cc0.0345 lb/in³ISO 1183-1
Melt Flow  4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 11 g/10 min
@Load 5.00 kg,
Temperature 190 °C
11 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ISO 868
Ball Indentation Hardness 52.0 MPa7540 psiISO 2039-1
Tensile Strength, Yield 27.0 MPa3920 psiISO 527-1,-2
Elongation at Yield 8.0 %8.0 %ISO 527-1,-2
Tensile Modulus 1.20 GPa174 ksiISO 527-1,-2
Charpy Impact, Notched  0.400 J/cm²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
Type 1, Edgewise, Notch A; ISO 179
 0.450 J/cm²
@Temperature -30.0 °C
2.14 ft-lb/in²
@Temperature -22.0 °F
Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 73.0 °C163 °FB50; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 250 °C356 - 482 °F
 
Descriptive Properties
Ball Indentation Hardness (MPa)H 132/30
FNCT (hrs)4.5ISO 16770, 6.0 MPa, 2% Arkopal N100, 50°C
Processing Methodinjection molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hostalen GD 7255 High Density Polyethylene (HDPE), Injection Molded
LyondellBasell Alathon® M5562 High Density Polyethylene
LyondellBasell Alathon® M6580 High Density Polyethylene
LyondellBasell Hostalen 5231H High Density Polyethylene (HDPE), Injection Molded
LyondellBasell Hostalen ACP 5331H High Density Polyethylene (HDPE), Injection Molded

PEQT8483 / 220118

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.