MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hostalen ACP 5331H High Density Polyethylene (HDPE), Injection Molded
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Hostalen ACP 5331 H is a state of the art HDPE resin, produced by latest Hostalen ACP technology. Hostalen ACP 5331 H is easy processable on injection molding and compression molding equipment. Exceptional organoleptic properties and a good balance of stiffness, toughness and environmental stress cracking resistance make Hostalen ACP 5331 H the choice of customers for the production of closures for sparkling water, CSD and many other types of food and nonfood caps and closures as well as tube shoulders. Applications: Caps & Closures, Collapsible Tubes

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.953 g/cc0.0344 lb/in³ISO 1183-1
Melt Flow  2.1 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.1 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 6.3 g/10 min
@Load 5.00 kg,
Temperature 190 °C
6.3 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6262ISO 868
Ball Indentation Hardness 51.0 MPa7400 psiISO 2039-1
Tensile Strength, Yield 30.0 MPa4350 psiISO 527-1,-2
Elongation at Yield 10 %10 %ISO 527-1,-2
Tensile Modulus 1.15 GPa167 ksiISO 527-1,-2
Charpy Impact, Notched  0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 75.0 °C167 °FB50; ISO 306
 
Descriptive Properties
FNCT (hrs)>9ISO 16770, 6.0 MPa, 2% Arkopal N100, 50°C
Processing MethodInjection Molding, compression molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hostalen ACP 6541A UV High Density Polyethylene (HDPE), Injection Molded
LyondellBasell Hostalen GC 7258 High Density Polyethylene (HDPE), Injection Molded
LyondellBasell Hostalen GC 7260 LS High Density Polyethylene (HDPE), Injection Molded
LyondellBasell Hostalen 5231H High Density Polyethylene (HDPE), Injection Molded
LyondellBasell Hostalen GC 7260 High Density Polyethylene (HDPE), Injection Molded

PEQT8449 / 220084

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.