MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond EP42HT-2LTE Two Component Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Very good temperature and chemical resistance
  • Convenient handling
  • Low shrinkage upon curing
  • Outstanding dimensional stability
Product Description: Master Bond EP42HT-2LTE is an innovative, two component epoxy system with an ultra low coefficient of thermal expansion. It can be used as an adhesive, sealant, coating and, in some cases, as a casting system. EP42HT-2LTE has a forgiving 100 to 40 mix ratio by weight, or a 100 to 50 mix ratio by volume. After mixing, the consistency is that of a paste with some flow. It will cure at room temperature in 4-7 days or more quickly at elevated temperatures, e.g. 4-6 hours at 150-200°F. However, to optimize properties, the recommended cure is overnight at room temperature followed by 3-5 hours at 150-200°F. The mainstay property of this epoxy system is its exceptionally low coefficient of expansion of 9-12 x 10-6 in/in/°C. It has an array of other highly desirable properties including stellar electrical insulation, very good chemical resistance and unsurpassed dimensional stability. This epoxy will bond well to a wide variety of substrates, including metals, composites, ceramics, glass and many plastics. It is also noteworthy for its low linear (<0.01%) and volumetric (<0.1%) shrinkage. The latter property is particularly useful in potting and encapsulation applications. Also, the compound allows for precise alignment with minimal fixturing and simple curing. Its service temperature range is from -60°F to +300°F. The color of Part A is light cream and Part B is similar, but slightly darker. EP42HT-2LTE and its very special property profile allows it to be a desirable selection for the more challenging electronic, aerospace, optical and specialty OEM applications. EP42HT-2LTE passes NASA low outgassing tests and is recommended for applications involving vacuums, optics and other usages that require this important property.

Product Advantages:

  • Non-critical 100 to 40 mix ratio by weight or 100 to 50 by volume
  • Easy application: only contact pressure required while curing; adhesive spreads readily
  • Highly reliable electrical insulator
  • High degree of dimensional stability
  • Desirably low shrinkage
  • Extraordinarily low coefficient of thermal expansion

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.70 g/cc2.70 g/ccPart B
 2.87 g/cc2.87 g/ccPart A
Viscosity 2000 - 6000 cP2000 - 6000 cPPart B
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 85 - 9085 - 90
Tensile Strength 41.4 - 48.3 MPa6000 - 7000 psi
Tensile Modulus 3.79 - 4.48 GPa550 - 650 ksi
Compressive Strength 179 - 193 MPa26000 - 28000 psi
Adhesive Bond Strength 4.83 - 6.21 MPa700 - 900 psiTensile lap, Aluminum to Aluminum
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 4.4
@Frequency 60 Hz
4.4
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.00 - 12.0 µm/m-°C5.00 - 6.67 µin/in-°F
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  240 - 360 min
@Temperature 65.6 - 93.3 °C
4.00 - 6.00 hour
@Temperature 150 - 200 °F
 5760 - 10100 min
@Temperature 23.9 °C
96.0 - 168 hour
@Temperature 75.0 °F
Working Life 60.0 - 90.0 min60.0 - 90.0 minAfter mixing, 100 g batch
Shelf Life 6.00 - 12.0 Month
@Temperature <=23.9 °C
6.00 - 12.0 Month
@Temperature <=75.0 °F
in original, unopened containers
 
Descriptive Properties
Cure Scheduleovernight at 75°Ffollowed by 3-5 hours at 150-200°F
Mixing Ratio100:40 by weightParts A to B
 100:50 by volumeParts A to B
Viscositymoderately flowable pastemixed
 pastePart A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Atom Adhesives AA-DUCT 905 Epoxy Adhesive
Master Bond EP48TC Two Part Epoxy Adhesive
Master Bond Supreme 42HT-2 Toughened Epoxy Resists Thermal Cycling
Overview of materials for Epoxy, Electrically Conductive
Master Bond EP29LPSP Low Outgassing, Optically Clear Two Component Epoxy

PMASTM882 / 185475

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.