MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Cabot STERLING® SO-RC110 Reinforcing Carbon
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Performance Features: Through Cabot’s co-pelletization technology, STERLING SO-RC110 circular reinforcing carbon combines ISCC PLUS certified recovered carbon material with STERLING SO to deliver physical performance that is equivalent to ASTM N550 carbon black, maintaining high levels of quality consistency and processability in rubber compounds.

Typical Applications: STERLING SO-RC110 circular reinforcing carbon is particularly suited for rubber applications that require an increase in sustainable content without compromising rubber performance, and for rubber compounders desiring logistic simplicity. STERLING SO-RC110 circular reinforcing carbon is applicable in all applications where ASTM N550 type carbon black is used, such as: Tires - Sidewalls and undertread compounds in passenger car and light truck tires; Industrial Rubber Products - Extruded rubber articles like hoses and construction profiles; Engine mounts and belt inner layers; and Molded rubber parts

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity 50
@Temperature 100 °C
50
@Temperature 212 °F
ML (1+4)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 58.258.2
Tensile Strength 19.4 MPa2810 psi
Elongation at Break 475 %475 %
300% Modulus 11.0 MPa1600 psi
 
Descriptive Properties
Dynamic Properties0.075Max tan delta, 10 Hz, 60 °C
 1.62 MpaG’ 10%, 10 Hz, 60 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCABOT011 / 315746

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.