MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Abatron AboCast 8110-6/AboCure 8110-1 Flexible Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive, Flexible

Material Notes: This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applications include: bonding, laminating, casting, embedding, electrical potting, impregnating, coating, etc. It can be supplied in several variations to modify viscosity, reaction rate, color, most physical and chemical properties, and with many fillers to meet most requirements.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 2.5 %
@Time 7200 sec
boil; cured 2 hours @ 93°C
Viscosity 2000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75
@Temperature 75.0 °C
cured 2 hrs. @ 93°C
 83
@Temperature 25.0 °C
cured 2 hrs. @ 93°C
 87
@Temperature 0.000 °C
cured 2 hrs. @ 93°C
 90
@Temperature -60.0 °C
cured 2 hrs. @ 93°C
Tensile Strength, Ultimate 6285 psicured 2 hours @ 93°C
 8435 psicured 8 hours @ 93°C
Elongation at Break 11 %cured 8 hours @ 93°C
 13 %cured 2 hours @ 93°C
Shear Strength 1770 psi
@Temperature 75.0 °C
Tensile, Al/Al lap joint; cured 2 hours @ 93°C
 4190 psi
@Temperature 0.000 °C
Tensile, Al/Al lap joint; cured 2 hours @ 93°C
 6080 psi
@Temperature 25.0 °C
Tensile, Al/Al lap joint; cured 2 hours @ 93°C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 7.90e+7 ohm-cm
@Temperature 150 °C
cured 2 hours @ 93°C
 7.70e+8 ohm-cm
@Temperature 112 °C
cured 2 hours @ 93°C
 2.70e+9 ohm-cm
@Temperature 100 °C
cured 2 hours @ 93°C
 9.40e+14 ohm-cm
@Temperature 25.0 °C
cured 2 hours @ 93°C
 
Processing PropertiesOriginal ValueComments
Pot Life 22 min
@Temperature 25.0 °C
200 g
Gel Time 6.00 min
@Temperature 93.0 °C
10 g
 
Descriptive Properties
Parts by Weight (pbw)10.2AboCure 8110-1
 100AboCast 8110-6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Adhesive, Flexible
Abatron AboCast/AboCure 8110-2 Flexible Epoxy
Abatron AboCast 8110-7/AboCure 8110-1 Flexible Epoxy
Abatron AboCast 8110-2/AboCure 8110-1 Flexible Epoxy
3M Scotch-Weld™ TE100 Black Polyurethane Reactive Adhesive

PABC872 / 107856

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.