MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Free-Cutting Muntz Metal, UNS C37000, H80 (Cold Drawn 35%) Temper 38 mm tube
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Fair to excellent corrosion resistance. Excellent machinability. Combines good machinability with excellent hot formability.

Applications: automatic screw machine parts.

Test specimen: tube - 38mm OD x 3mm wall thickness.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.41 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell F 85
Hardness, Rockwell 30T 74
Tensile Strength, Ultimate 550 MPa
Tensile Strength, Yield 415 MPa
@Strain 0.5 %
Elongation at Break 6.0 %In 50 mm
Modulus of Elasticity 105 GPa
Poissons Ratio 0.346
Machinability 70 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 39.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000639 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.8 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.375 J/g-°C
Thermal Conductivity 120 W/m-K
@Temperature 20.0 °C
Melting Point 885 - 900 °C
Solidus 885 °C
Liquidus 900 °C
Annealing Point 800 - 1100 °F
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 425 - 600 °C
Hot-Working Temperature 625 - 800 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 59 - 62 %
Iron, Fe <= 0.15 %
Lead, Pb 0.90 - 1.4 %
Other, total <= 0.50 %
Zinc, Zn 39 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Copper, UNS C15735
Antimonial Admiralty Copper, UNS C44400, OSO25 Temper tubing
Overview of materials for Bronze
Mueller EcoStream™ C37000 Free Cutting Muntz Metal
Low-leaded brass, UNS C33500

MC37000b4 / 11252

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.