MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Free-Cutting Muntz Metal, UNS C37000, H80 (Cold Drawn 35%) Temper 38 mm tube
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Fair to excellent corrosion resistance. Excellent machinability. Combines good machinability with excellent hot formability.

Applications: automatic screw machine parts.

Test specimen: tube - 38mm OD x 3mm wall thickness.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.41 g/cc0.304 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell F 8585
Hardness, Rockwell 30T 7474
Tensile Strength, Ultimate 550 MPa79800 psi
Tensile Strength, Yield 415 MPa
@Strain 0.5 %
60200 psi
@Strain 0.5 %
Elongation at Break 6.0 %6.0 %In 50 mm
Modulus of Elasticity 105 GPa15200 ksi
Poissons Ratio 0.3460.346
Machinability 70 %70 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 39.0 GPa5660 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000639 ohm-cm
@Temperature 20.0 °C
0.00000639 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.8 µm/m-°C
@Temperature 20.0 - 300 °C
11.6 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.375 J/g-°C0.0896 BTU/lb-°F
Thermal Conductivity 120 W/m-K
@Temperature 20.0 °C
833 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 885 - 900 °C1630 - 1650 °F
Solidus 885 °C1630 °F
Liquidus 900 °C1650 °F
Annealing Point 427 - 593 °C800 - 1100 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 425 - 600 °C797 - 1110 °F
Hot-Working Temperature 625 - 800 °C1160 - 1470 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 59 - 62 %59 - 62 %
Iron, Fe <= 0.15 %<= 0.15 %
Lead, Pb 0.90 - 1.4 %0.90 - 1.4 %
Other, total <= 0.50 %<= 0.50 %
Zinc, Zn 39 %39 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper, UNS C15735
Antimonial Admiralty Copper, UNS C44400, OSO25 Temper tubing
Overview of materials for Bronze
Mueller EcoStream™ C37000 Free Cutting Muntz Metal
Low-leaded brass, UNS C33500

MC37000b4 / 11252

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.