MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

BYK Claytone® II Organophilic Bentonite
Categories: Ceramic; Clay; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Claytone II, an organoclay, is recommended as a rheological additive in oil based fluids and drilling muds. Claytone II is a high quality thixotrope suitable for use in a wide variety of oils and solvents. In addition to imparting excellent rheological properties, Claytone II increases the carrying capacity and hole cleaning capabilities of the mud. Additionally, temperature and emulsion stability will be increased and fluid loss decreased.

Uses & Advantages:

  • Use in all oil based drilling fluids requiring rheological modification.
  • Use in oil muds that are to be used as packer fluids or for stabilizer of stored muds.
  • Available in easy to handle 50 lb. bags.
  • Economical, convenient, and safe to handle, mix, and store.
  • Easily dispersed and free flowing.

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.417 g/cc0.0150 lb/in³loose
Particle Mesh Size 200 Mesh200 Mesh85%
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) 37 %
@Temperature 1000 °C
37 %
@Temperature 1830 °F
 
Descriptive Properties
Color/FormOff-White, Free Flowing powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BYK Bentolite® L3 Magnesium aluminum Silicate Additive
BYK Claytone® HT Rheological Additive
BYK Claytone® ER Organophilic Bentonite
BYK Claytone® EM Gellant for Oil Mud Systems
BYK Claytone® APA Rheological Additive

PBYK018 / 185015

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.