MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Zhejiang Juner PA-A6-6H High CTI Value Halogen-Free Environmental Protection Flame-Resistant and Reinforced Polyamide
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Mineral Reinforced, Impact Grade

Material Notes: Applications: Circuit Breaker, Base

Information provided by Zhejiang Juner New Materials Co, Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.55 g/ccGB/1033
Water Absorption 0.60 %23°C•24h
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 60.0 MPaGB/1040
Elongation at Break 2.0 %GB/1040
Flexural Strength 100 MPaGB/9341
Flexural Modulus 8.80 GPaGB/9341
Charpy Impact Unnotched 2.00 J/cm²IS0179-1:2000
Charpy Impact, Notched 0.500 J/cm²IS0179-1:2000
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmGB/1410
Comparative Tracking Index 550 VGB/4207
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 150 °CGB1634
Flammability, UL94 V-0GB/T2408
 
Processing PropertiesOriginal ValueComments
Processing Temperature 225 - 250 °C
Mold Temperature 60.0 - 90.0 °C
Drying Temperature 110 °C
@Time 18000 sec
Chute Hot-Wind
 110 °C
@Time 18000 sec
Horizontal Oven
 110 °C
@Time 7200 sec
Vacuum Pressure, -0.08 MPa
Injection Pressure 80.0 - 100 MPa
 
Descriptive Properties
Speed of Shoot, %35-80

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese SO.F.TER Nylfor B® B2 FR2/3A Polyamide 6
Zhejiang Juner PA-A5 Flame-Retardant & Mineral Reinforced PA6
Zhejiang Juner PA-A4 Flame-Retardant & Mineral Reinforced PA6
Röhm ACRYLITE® Soundstop BirdGuard, Acrylic
INEOS Styrolution Luran® S KR2858 G3 Acrylonitrile Styrene Acrylate (ASA)

PJUNER52 / 48565

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.