Zhejiang Juner PA-A5 Flame-Retardant & Mineral Reinforced PA6
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
Material Notes:
Applications: Mid-Grade CB
Information provided by Zhejiang Juner New Materials Co, Ltd.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.58
g/cc
0.0571
lb/in³
GB/1033
Water Absorption
0.60 %
0.60 %
23°C•24h
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
70.0
MPa
10200
psi
GB/1040
Flexural Strength
115
MPa
16700
psi
GB/9341
Charpy Impact Unnotched
2.80
J/cm²
13.3
ft-lb/in²
IS0179-1:2000
Charpy Impact, Notched
0.600
J/cm²
2.86
ft-lb/in²
IS0179-1:2000
Electrical Properties
Metric
English
Comments
Comparative Tracking Index
350
V
350
V
GB/4207
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
155
°C
311
°F
GB1634
Flammability, UL94
V-0
V-0
GB/T2408
Flammability Test
30
30
Flame Remainder (%); GB/9345
Processing Properties
Metric
English
Comments
Processing Temperature
225
-
255
°C
437
-
491
°F
Mold Temperature
40.0
-
100
°C
104
-
212
°F
Drying Temperature
110
°C
@Time 7200 sec
230
°F
@Time 2.00 hour
Vacuum Pressure, -0.08 MPa
120
°C
@Time 18000 sec
248
°F
@Time 5.00 hour
Chute Hot-Wind
120
°C
@Time 21600 sec
248
°F
@Time 6.00 hour
Horizontal Oven
Injection Pressure
40.0
-
90.0
MPa
5800
-
13100
psi
Descriptive Properties
Speed of Shoot, %
30-80
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Celanese SO.F.TER Nylfor B® B2 FR2/3A Polyamide 6
Zhejiang Juner PA-A6-6H High CTI Value Halogen-Free Environmental Protection Flame-Resistant and Reinforced Polyamide
Zhejiang Juner PA-A4 Flame-Retardant & Mineral Reinforced PA6
Celanese SO.F.TER Nylfor B® B2 GF/30 FR2/3A Polyamide 6
Celanese SO.F.TER Nylfor B® B2 FR1/2A Polyamide 6
PJUNER17 / 48530
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.