Temper: As Sand Cast Fabrication Properties: Excellent Suitability– Soldering; Fair Suitability – Brazing; Poor Suitability – Capacity for Being Cold Worked, Capacity for Being Hot Formed Typical uses: Cu based devices for lead-free water applications; Lead-free defined as Calif. AB 1953 max. .25% lead content; Lead-free, dezincification resistant for potable water components; valves, fittings, pumps, meters Applicable Specifications: As Sand Cast – Valves ASTM B763/B763M, ASTM B584; Ingot – ASTM B30 |