MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ATI Allegheny Ludlum 430 Ferritic Stainless Steel
Categories: Metal; Ferrous Metal; Ferritic; Stainless Steel; T 400 Series Stainless Steel

Material Notes:

Characteristics:oxidation resistant at elevated temperatures, corrosion resistance approaching nickel-bearing stainless steels in mildly corrosive environments, ductile, does not work harden readily.

Forms:plates, sheets, strip, foil.

Applications:interior and exterior trim, sinks, counter tops, dish washers, range hoods, flatware, roofing, siding, and restaurant equipment.

Information provided by Allegheny Ludlum

Key Words: UNS S43000
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 7.70 g/cc7.70 g/cc
Density 7.70 g/cc0.278 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 75 - 83
@Thickness 1.02 - 2.92 mm
75 - 83
@Thickness 0.0400 - 0.115 in
Hardness, Rockwell 30T 62 - 70
@Thickness 0.508 - 1.52 mm
62 - 70
@Thickness 0.0200 - 0.0600 in
Tensile Strength, Ultimate  455 - 538 MPa
@Thickness 1.02 - 2.92 mm
66000 - 78000 psi
@Thickness 0.0400 - 0.115 in
 483 - 545 MPa
@Thickness 0.508 - 1.52 mm
70100 - 79000 psi
@Thickness 0.0200 - 0.0600 in
Tensile Strength, Yield  303 - 372 MPa
@Strain 0.2 %,
Thickness 0.508 - 1.52 mm
43900 - 54000 psi
@Strain 0.2 %,
Thickness 0.0200 - 0.0600 in
 296 - 386 MPa
@Strain 0.2 %,
Thickness 1.02 - 2.92 mm
42900 - 56000 psi
@Strain 0.2 %,
Thickness 0.0400 - 0.115 in
Elongation at Break  21 - 34 %
@Thickness 0.508 - 1.52 mm
21 - 34 %
@Thickness 0.0200 - 0.0600 in
 23 - 37 %
@Thickness 1.02 - 2.92 mm
23 - 37 %
@Thickness 0.0400 - 0.115 in
Creep Strength  6.90 MPa
@Temperature 760 °C,
Time 3.60e+7 sec
1000 psi
@Temperature 1400 °F,
Time 10000 hour
 69.0 MPa
@Temperature 538 °C,
Time 3.60e+7 sec
10000 psi
@Temperature 1000 °F,
Time 10000 hour
Fatigue Strength 159 - 243 MPa
@# of Cycles 1.00e+7
23100 - 35200 psi
@# of Cycles 1.00e+7
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0000600 ohm-cm
@Temperature 20.0 °C
0.0000600 ohm-cm
@Temperature 68.0 °F
 0.0000675 ohm-cm
@Temperature 100 °C
0.0000675 ohm-cm
@Temperature 212 °F
 0.0000770 ohm-cm
@Temperature 200 °C
0.0000770 ohm-cm
@Temperature 392 °F
 0.0000925 ohm-cm
@Temperature 400 °C
0.0000925 ohm-cm
@Temperature 752 °F
 0.000105 ohm-cm
@Temperature 600 °C
0.000105 ohm-cm
@Temperature 1110 °F
 0.000115 ohm-cm
@Temperature 800 °C
0.000115 ohm-cm
@Temperature 1470 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.3 µm/m-°C
@Temperature 20.0 - 100 °C
5.72 µin/in-°F
@Temperature 68.0 - 212 °F
 11.2 µm/m-°C
@Temperature 20.0 - 500 °C
6.22 µin/in-°F
@Temperature 68.0 - 932 °F
 11.9 µm/m-°C
@Temperature 20.0 - 787 °C
6.61 µin/in-°F
@Temperature 68.0 - 1450 °F
Specific Heat Capacity 0.460 J/g-°C
@Temperature 0.000 - 100 °C
0.110 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity  23.86 W/m-K
@Temperature 20.0 - 100 °C
165.6 BTU-in/hr-ft²-°F
@Temperature 68.0 - 212 °F
 25.96 W/m-K
@Temperature 20.0 - 500 °C
180.2 BTU-in/hr-ft²-°F
@Temperature 68.0 - 932 °F
Melting Point 1425 - 1510 °C2597 - 2750 °F
Solidus 1425 °C2597 °F
Liquidus 1510 °C2750 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.12 %<= 0.12 %
Chromium, Cr 16 - 18 %16 - 18 %
Iron, Fe >= 79.31 %>= 79.31 %As Remainder
Manganese, Mn <= 1.0 %<= 1.0 %
Molybdenum, Mo <= 0.50 %<= 0.50 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
316 Stainless Steel, annealed and cold drawn bar
AK Steel 430 Ferritic Stainless steel
409 Stainless Steel
Eagle Brass 430 Ferritic Stainless Steel, Annealed
Haynes 718 alloy, cold rolled, solution-treated and aged sheet

NL1009 / 17777

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.