MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
AiResist 213 Cobalt Alloy (AR-213)
Categories: Metal; Nonferrous Metal; Cobalt Alloy

Material Notes: Resistant to hot corrosion; typical applications: sheets, tubing. Precipitation Hardening.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 315 MPa
@Temperature 870 °C
 485 MPa
@Temperature 760 °C
 960 MPa
@Temperature 650 °C
 1120 MPa
@Temperature 21.0 °C
Tensile Strength, Yield 220 MPa
@Strain 0.2 %,
Temperature 870 °C
 385 MPa
@Strain 0.2 %,
Temperature 760 °C
 425 MPa
@Strain 0.2 %,
Temperature 650 °C
 625 MPa
@Strain 0.2 %,
Temperature 21.0 °C
Elongation at Break 14 %
@Temperature 21.0 °C
 28 %
@Temperature 650 °C
 47 %
@Temperature 760 °C
 55 %
@Temperature 870 °C
Rupture Strength 2800 psi
@Temperature 1090 °C,
Time 360000 sec
 3500 psi
@Temperature 982 °C,
Time 3.60e+6 sec
 5000 psi
@Temperature 982 °C,
Time 360000 sec
 13000 psi
@Temperature 816 °C,
Time 3.60e+6 sec
 20000 psi
@Temperature 816 °C,
Time 360000 sec
 65000 psi
@Temperature 649 °C,
Time 360000 sec
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 3.5 %
Carbon, C 0.18 %
Chromium, Cr 19 %
Cobalt, Co 66 %
Tantalum, Ta 6.5 %
Tungsten, W 4.7 %
Yttrium, Y 0.10 %
Zirconium, Zr 0.15 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Grade 18Ni (350) Maraging Steel nominal annealed properties
Arcam ASTM F-75 Cobalt Chrome Alloy
AK Steel 316L Austenitic Stainless steel
Sylvania SA201 Tungsten & Chrome Based Thermal Spray Powder
Overview of materials for Maraging Steel

NZ988 / 170617

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.