MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman Alcryn® 2165 TR Melt Processable Rubber
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: The 2100 Series grades of Alcryn® offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn®. The new 2100 grades bond to polycarbonate, ABS, polycarbonate/ABS alloys, SAN, ASA, copolyester elastomers and TPUs, as well as both flexible and rigid PVC. The 2100 series
  • is high flow in general plastic processing
  • is designed for injection molding and overmolding
  • is excellent for complex extrusions
  • is excellent for co-extrusions

  • injection molded and overmolded parts
  • soft touch handles and grips on appliance and tool applications
  • automotive interior applications
  • noise and vibration deadening
  • seals and gaskets for automotive insert molding
  • window and door weather stripping (and other complex profile extrusions)
  • coated fabrics and sheet goods
  • wire and cable jackets
  • tubing and hose
  • blow molded parts

Information provided by Advanced Polymer Alloys

Former product line of Advanced Polymer Alloys (APA), acquired by A. Schulman in 2014.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/ccASTM D471
Viscosity 232000 cP
@Shear Rate 300 1/s,
Temperature 190 °C
ASTM D3835
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60After 7 days at 125°C; ASTM D573
 66ASTM D2240
Tensile Strength at Break 1698 psiAfter 7 days at 125°C; ASTM D573
 1769 psiASTM D412
Elongation at Break 518.7 %After 7 days at 125°C; ASTM D573
 570 %ASTM D412
100% Modulus 0.450 ksi
@Strain 100 %
ASTM D412
 0.4905 ksi
@Strain 100 %
After 7 days at 125°C; ASTM D573
Graves Tear Strength 262.5 pli
@Temperature 24.0 °C
Die C; ASTM D624
Compression Set 34 %
@Temperature 24.0 °C,
Time 79200 sec
ASTM D395
 83 %
@Temperature 100 °C,
Time 79200 sec
ASTM D395
Tensile Set 13 %ASTM D412
 
Processing PropertiesOriginal ValueComments
Processing Temperature 177 °C
 
Descriptive Properties
Fluid Resistance - Volume Change, % (ASTM D471)-16After 7 Days in ASTM Oil No. 1 At 212°F (100°C)
 19After 7 Days in ASTM Ref. Fuel no. B at 75°F (24°C)
 7After 7 Days in Water at 212°F (100°C)
 9After 7 Days in IRM 903 Oil No. 3 at 212°F (100°C)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Uniprene® UN-2598D Thermoplastic Vulcanizate
Covestro Makrolon® 6357 Polycarbonate, Flame Retardant Grade
INEOS Styrolution Luran® S 767KE Acrylonitrile Styrene Acrylate (ASA)
LG Chemical LI968P ASA, Co-Extrusion
Kuraray SEPTON® S1001 Thermoplastic Rubber

PAPA009A / 24076

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.