MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LI968P ASA, Co-Extrusion
Categories: Polymer; Thermoplastic; ASA Polymer

Material Notes: Good Weatherability

Applications: PC-ASA Alloy

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0070 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 11 g/10 min
@Load 10.0 kg,
Temperature 220 °C
11 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 102102ASTM D785
Tensile Strength, Yield 47.0 MPa
@Thickness 3.20 mm
6810 psi
@Thickness 0.126 in
50 mm/min; ASTM D638
Elongation at Break >= 15 %
@Thickness 3.20 mm
>= 15 %
@Thickness 0.126 in
50 mm/min; ASTM D638
Elongation at Yield >= 6.0 %
@Thickness 3.20 mm
>= 6.0 %
@Thickness 0.126 in
50 mm/min; ASTM D638
Tensile Modulus 2.10 GPa
@Thickness 3.20 mm
305 ksi
@Thickness 0.126 in
50 mm/min; ASTM D638
Flexural Strength 74.0 MPa
@Thickness 3.20 mm
10700 psi
@Thickness 0.126 in
15 mm/min; ASTM D790
Flexural Modulus 2.40 GPa
@Thickness 3.20 mm
348 ksi
@Thickness 0.126 in
15 mm/min; ASTM D790
Izod Impact, Notched  0.300 J/cm
@Thickness 3.20 mm,
Temperature -30.0 °C
0.562 ft-lb/in
@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
 0.300 J/cm
@Thickness 6.40 mm,
Temperature -30.0 °C
0.562 ft-lb/in
@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
 1.30 J/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
2.44 ft-lb/in
@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
 1.70 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
3.18 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C
@Thickness 6.40 mm
187 °F
@Thickness 0.252 in
Unannealed, Edgewise; ASTM D648
Vicat Softening Point 92.0 °C
@Load 5.10 kg
198 °F
@Load 11.2 lb
50°C/h; ASTM D1525
 
Processing PropertiesMetricEnglishComments
Zone 1 190 - 200 °C374 - 392 °F
Zone 2 200 - 220 °C392 - 428 °F
Zone 3 210 - 230 °C410 - 446 °F
Zone 4 210 - 230 °C410 - 446 °F
Adapter Temperature 210 - 230 °C410 - 446 °F
Die Temperature 210 - 250 °C410 - 482 °F
Melt Temperature 200 - 230 °C392 - 446 °F
Roll Temperature 70.0 - 90.0 °C158 - 194 °FMiddle
 70.0 - 90.0 °C158 - 194 °FTop
 70.0 - 100 °C158 - 212 °FBottom
Drying Temperature 80.0 - 90.0 °C
@Time 7200 - 10800 sec
176 - 194 °F
@Time 2.00 - 3.00 hour
Moisture Content >= 0.10 %>= 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Luran® S 767KE Acrylonitrile Styrene Acrylate (ASA)
INEOS Styrolution Luran® S 797SE Q440 Acrylonitrile Styrene Acrylate (ASA)
Covestro Makrolon® 6357 Polycarbonate, Flame Retardant Grade
LG Chemical LI968W Co-Extrusion ASA
LG Chemical LI970 Co-Extrusion ASA

PLHCHEM9975 / 239491

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.