MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik VESTAMID® HTplus M1634 black Polyphthalamide (PPA), 40% Glass Fiber Reinforced  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 40% Glass Fiber Reinforced

Material Notes: Glass fiber-reinforced polyphthalamide compound for drinking water applications. VESTAMID® HTplus M1634 black is a glass fiber-reinforced (40%), heat-stabilized polyphthalamide compound (PPA). This compound is especially suitable for manufacturing injection molded parts for metal substitution in industrial, household and sanitary equipment in contact with drinking water. Approvals for drinking water: KTW (up to 60°C), WRAS (up to 60°C).,NSF61 (up to 60°C), ACS, DVGW code of practice W270. VESTAMID® HTplus M1634 black is supplied as cylindrical pellets in polyethylene packaging. Drying at 120°C for at least 4 hours before processing is recommended.

Property data for dry samples.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.54 g/cc0.0556 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 205 MPa29700 psiISO 527
Elongation at Break 0.70 %0.70 %ISO 527
Tensile Modulus 14.3 GPa2070 ksiISO 527
Flexural Modulus 13.2 GPa1910 ksiISO 178
Charpy Impact Unnotched  3.40 J/cm²
@Temperature -40.0 °C
16.2 ft-lb/in²
@Temperature -40.0 °F
Complete Break; ISO 179/1eU
 4.70 J/cm²
@Temperature 23.0 °C
22.4 ft-lb/in²
@Temperature 73.4 °F
Complete Break; ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
Complete Break; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 330 °C626 °F0
Deflection Temperature at 0.46 MPa (66 psi) 305 °C581 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 290 °C554 °FISO 75-1/-2
Vicat Softening Point 284 °C543 °FMethod B: 10 N, 50 K/h; ISO 306
 308 °C586 °FMethod A: 10 N, 50 K/h; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 330 °C626 °FTest condition for mold shrinkage
Mold Temperature 160 °C320 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK838 / 243047

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.