MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Datum Alloys 304TA Stainless Steel Thin Foil
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: This precision 304 stainless thin foil has exceptional shape control when laser cutting and etching. It comes in a wide range of dimensions. Material produced to JIS standard G 4313 for 304 H.

Tension annealing (TA) is a specialized process that relieves internal stress while the strip is under tension. This creates the mechanical properties of a hard temper without the rolling stresses typically induced into such material. This results in a hard material that can be laser cut and etched without shape deformation.

Information provided by Datum Alloys.

Vendors: Datum Alloys is the leader in precision alloys for niche applications such as advanced stainless steel foils for the Surface Mount Technology (SMT) industry and of nickel and nickel plated tags used in the manufacture of battery packs. Call +1 607 239 6274 or visit datumalloys.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.93 g/cc0.286 lb/in³
Thickness 20.3 - 508 microns0.800 - 20.0 mil
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 370370
Tensile Strength >= 1130 MPa>= 164000 psi
Tensile Strength, Yield >= 880 MPa
@Strain 0.2 %
>= 128000 psi
@Strain 0.2 %
Tensile Modulus 197 GPa28600 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000720 ohm-cm0.0000720 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.3 µm/m-°C
@Temperature 0.000 - 100 °C
9.61 µin/in-°F
@Temperature 32.0 - 212 °F
Specific Heat Capacity 0.502 J/g-°C
@Temperature 0.000 - 100 °C
0.120 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity 16.3 W/m-K
@Temperature 100 °C
113 BTU-in/hr-ft²-°F
@Temperature 212 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.080 %<= 0.080 %
Chromium, Cr 18 - 20 %18 - 20 %
Iron, Fe 66.5 - 74 %66.5 - 74 %as balance
Manganese, Mn <= 2.0 %<= 2.0 %
Nickel, Ni 8.0 - 10.5 %8.0 - 10.5 %
Phosphorus, P <= 0.050 %<= 0.050 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
304 Stainless Steel
AISI Type 304L Stainless Steel
Overview of materials for T 300 Series Stainless Steel
304 Stainless Steel (UNS S30400); Full Hard
Cast Stainless Steel 440C, ASTM A276

NDATUM90 / 198185

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.