MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol Estane® AG 8451 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Type: Estane® AG 8451 is a polyether based aliphatic (TPU) specifically formulated to be used as an adhesive interlayer film. AG-8451 is an excellent general purpose polymer for all optical allphatic applications.

Features: This polymer works over a broad range of processing temperatures with excellent laminating results.

Uses: Adhesive interlayer for glass-clad polycarbonate without a surface primer.

Available in Americas

Information Provided by The Lubrizol Corporation

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 7000 psiASTM D412
Elongation at Break 475 %ASTM D412
100% Modulus 0.500 ksi
@Strain 100 %
ASTM D412
200% Modulus 1.20 ksi
@Strain 200 %
ASTM D412
300% Modulus 2.00 ksi
@Strain 300 %
ASTM D412
Tear Strength 320 pliDie C; ASTM D624
Compression Set 23 %
@Temperature 22.0 °C,
Time 79200 sec
ASTM D395-98
 95 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395-98
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -60.0 °CDSC
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.4962ASTM D542-95
Haze 0.00 - 0.30 %ASTM D1003
Yellow Index <= 1.0 %ASTM D1925
Transmission, Visible 85 - 95 %ASTM D1003
 
Descriptive Properties
TMA Peak (°C)88
TMA Range (°C)65-130

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Estane® AG 9550 Thermoplastic Polyurethane
Austin Novel Materials Texalan® 598A Polyether-based TPU
Austin Novel Materials Texalan® 698A Polyester and Polyether based TPU
Lubrizol Estane® AG 4350 Thermoplastic Polyurethane
Taiwan PU Corporation TPU-EH95 High Hydrolysis Resistance, Extrusion Molding Polyether Base TPU

PNOVEON565 / 121456

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.