MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Estane® AG 9550 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Type: Estane® AG 9550 is a polyether based aliphatic polyurethane designed for flat die extrusion into film and sheet products.

Features: Very tough, high modulus, high tear and tensile properties that will impart good impact resistance to bullet-resistant applications. Excellent impact and UV resistance.

Uses: Designed for the lamination of glass to glass laminates with exposed edges.

Information Provided by The Lubrizol Corporation

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 62.1 MPa9000 psiASTM D412
Elongation at Break 375 %375 %ASTM D412
100% Modulus 12.4 MPa
@Strain 100 %
1800 psi
@Strain 100 %
ASTM D412
200% Modulus 17.2 MPa
@Strain 200 %
2500 psi
@Strain 200 %
ASTM D412
300% Modulus 29.6 MPa
@Strain 300 %
4300 psi
@Strain 300 %
ASTM D412
Tear Strength 77.1 kN/m440 pliDie C; ASTM D624
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -35.0 °C-31.0 °FDSC
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4991.499ASTM D542-95
Haze 0.30 %0.30 %ASTM D1003
Yellow Index <= 1.0 %<= 1.0 %ASTM D1925
Transmission, Visible 90 %90 %ASTM D1003
 
Descriptive Properties
TMA Peak (°C)155
TMA Range (°C)90-200

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Estane® ALR CL87A Thermoplastic Polyurethane
Lubrizol Estane® ALR CL57D Thermoplastic Polyurethane
Lubrizol Estane® R190A Thermoplastic Polyurethane
Lubrizol Estane® AG 8451 Thermoplastic Polyurethane
Lubrizol Estane® ALR CL60D Thermoplastic Polyurethane

PNOVEON566 / 121457

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.