MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo MAGNUM™ 3904 Smooth Acrylonitrile Butadiene Styrene (ABS) Resin
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: MAGNUM™ 3904 is an extrusion/thermoforming resin developed for high impact and other technical applications. The mass (continuous process) ABS technology of Styron ensures an ABS technology of Styron ensures an ABS resin that combines excellent processabiltiy with a stable light base color that is ideal for self-coloring. The new MAGNUM ‘Smooth Series’ resins have an ultra low particulate content, which results in a good surface finish that will enable our customers to produce parts with excellent aesthetics at a low total cost.

Applications:

  • Transportation
  • Protective covers
  • Sanitary ware
  • Marine
  • Signage
  • Recreation vehicles
  • Furnishings
Automotive Specifications:
  • CHRYSLER MS-DB-300 CPN4432

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183/B
Apparent Bulk Density 0.650 g/cc0.0235 lb/in³ISO 60
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inISO 294-4
Melt Flow 4.7 g/10 min
@Load 10.0 kg,
Temperature 220 °C
4.7 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield  37.0 MPa
@Thickness 3.20 mm
5370 psi
@Thickness 0.126 in
Injection Molded; ISO 527-2/50
 39.0 MPa
@Thickness 3.20 mm
5660 psi
@Thickness 0.126 in
Injection Molded; ISO 527-2/100
Elongation at Yield  2.6 %
@Thickness 3.20 mm
2.6 %
@Thickness 0.126 in
Injection Molded; ISO 527-2/50
 2.8 %
@Thickness 3.20 mm
2.8 %
@Thickness 0.126 in
Injection Molded; ISO 527-2/100
Tensile Modulus 1.82 GPa
@Thickness 3.20 mm
264 ksi
@Thickness 0.126 in
Injection Molded; ISO 527-2
Flexural Strength 58.0 MPa
@Thickness 3.20 mm
8410 psi
@Thickness 0.126 in
3-points, 2 mm/min, Injection Molded; ISO 178
Flexural Modulus 1.90 GPa
@Thickness 3.20 mm
276 ksi
@Thickness 0.126 in
3-points, 2 mm/min, Injection Molded; ISO 178
Izod Impact, Notched (ISO)  17.0 kJ/m²
@Temperature -30.0 °C
8.09 ft-lb/in²
@Temperature -22.0 °F
Injection Molded; ISO 180/A
 42.0 kJ/m²
@Temperature 23.0 °C
20.0 ft-lb/in²
@Temperature 73.4 °F
Injection Molded; ISO 180/A
Charpy Impact, Notched  1.20 J/cm²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
Injection Molded; ISO 179/2C
 1.80 J/cm²
@Temperature -30.0 °C
8.57 ft-lb/in²
@Temperature -22.0 °F
Injection Molded; ISO 179/1eA
 2.20 J/cm²
@Temperature 23.0 °C
10.5 ft-lb/in²
@Temperature 73.4 °F
Injection Molded; ISO 179/2
 3.70 J/cm²
@Temperature 23.0 °C
17.6 ft-lb/in²
@Temperature 73.4 °F
Injection Molded; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 97.0 °C207 °FAnnealed; ISO 75-2/A
Vicat Softening Point 97.0 °C207 °FISO 306/B50
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
Flame Spread 40.0 mm/min1.57 in/minISO 3795

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo MAGNUM™ 3904 Acrylonitrile Butadiene Styrene (ABS) Resin
Trinseo MAGNUM™ 3904 Ultra Smooth ABS
Daicel CEVIAN® S5230 30% GF PC/ABS alloy
Trinseo Magnum™ 8391 MED Acrylonitrile Butadiene Styrene (ABS) Resin
Applied Nanostructured Solutions PC/ABS - Carbon NanoStructure Chopped Fiber Composite

PZZDWST073 / 142282

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.