MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lubrizol Pearlstick™ 5719 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Type: Pearlstick™ 5719 TPU is a Polyester-Type Thermoplastic Polyurethane (TPU).

Features: High tensile strength, low temperature flexibility, and high adhesion to various substrates such as PET, PVC and various fabrics.

Uses: Fabric coating and audio tape binder, inks and solution cast pigment dispersion media.

Information provided by The 159 Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Brookfield Viscosity 200 cP200 cP15% T.S. in THF, RVT Spindle #2, 20 RPM, 23°C
 1500 cP1500 cP15% T.S. in Cyclohexanone, RVT Spindle #2, 20 RPM, 23°C
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080ASTM D2240
Tensile Strength 50.3 MPa7300 psiASTM D-412/D-638
Elongation at Break 430 %430 %ASTM D-412/D-638
100% Modulus 2.30 MPa
@Strain 100 %
334 psi
@Strain 100 %
ASTM D-412/D-638
300% Modulus 5.90 MPa
@Strain 300 %
856 psi
@Strain 300 %
ASTM D-412/D-638
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 35.0 °C95.0 °FASTM D-1525
Glass Transition Temp, Tg 19.0 °C66.2 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol ESTANE® 5703 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 5719 Ester Based Thermoplastic Polyurethane
Ecomass® 4703BI62 Filled Polyurethane, Injection Molding
Huntsman IROGRAN® A 98 H 4661 Polyester-Based TPU-Injection Molding Grade
Huntsman IROGRAN® A 95 H 4678 Polyester-Based TPU-Injection Molding Grade

PLUBR5014 / 238884

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.