System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Ecomass® 4703BI62 Filled Polyurethane, Injection Molding
Categories:
Polymer
;
Thermoplastic
;
Polyurethane, TP
Material Notes:
Moderate Specific Gravity, Filled Polyurethane (TPU), Good Flexibility, Product Form - Pellets
Processing Method:
Injection Molding
Nontoxic alternative to Lead, radiation shielding applications
Information provided by Technical Polymers.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
2.20
g/cc
2.20
g/cc
ASTM D792
Linear Mold Shrinkage
0.0070
-
0.0090
cm/cm
0.0070
-
0.0090
in/in
ASTM D955
Mechanical Properties
Metric
English
Comments
Tensile Strength
20.7
MPa
3000
psi
ASTM D638
Elongation at Break
225 %
225 %
ASTM D638
Tensile Modulus
0.565
GPa
82.0
ksi
ASTM D638
Flexural Strength
42.7
MPa
6200
psi
ASTM D790
Flexural Modulus
0.145
GPa
21.0
ksi
ASTM D790
Izod Impact, Notched
2.67
J/cm
5.00
ft-lb/in
ASTM D256
Processing Properties
Metric
English
Comments
Melt Temperature
204
-
221
°C
400
-
430
°F
Mold Temperature
10.0
-
26.7
°C
50.0
-
80.0
°F
Drying Temperature
82.2
°C
180
°F
do not over dry
Dry Time
2
hour
2
hour
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Huntsman IROGRAN® A 95 H 4678 Polyester-Based TPU-Injection Molding Grade
Lubrizol Advanced Materials Pearlbond® 580 Thermoplastic Polyurethane
Lubrizol Advanced Materials PEARLCOAT® 163K Thermoplastic Polyurethane Elastomer
Lubrizol Estane® BCXA07 Thermoplastic Polyurethane
Lubrizol LifeSciences Tecoflex® EG-85A TPU - Clear
PECOM918 / 133731
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.