MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Australian Jarrah Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Data is based on small, clear, air-dried samples unless specified.
Usual surface texture: Medium
Dimensional changes when dried lumber is subjected to variations in humidity during service: Medium
Resistance to fungal decay (Heartwood in ground contact): Very Durable (Over 25 years)
Resistance to penetration by preservatives: Extremely resistant
Common Applications: Heavy constructional work. Flooring

Key Words: Eucalyptus marginata; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.670 g/ccGreen
Density 0.770 g/ccAir Dry (12-15% Moisture Content)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 5700 NSide Hardness, Green
 8500 NSide Hardness, 12% Moisture
Modulus of Rupture 0.0683 GPaStatic Bending, Green
 0.1117 GPaStatic Bending, 12% Moisture
Flexural Modulus 10200 MPaStatic Bending, Green
 13000 MPaStatic Bending, 12% Moisture
Compressive Strength 35.8 MPaParallel to Grain, Green
 61.2 MPaParallel to Grain, 12% Moisture
Machinability 10 %Difficult Relative to Other Wood
Shear Strength 9.10 MPaParallel to Grain, Green
 14.7 MPaParallel to Grain, 12% Moisture
 
Thermal PropertiesOriginal ValueComments
Shrinkage 5.0 %Radial; Green to Zero Moisture
 7.7 %Radial Shrinkage Green to Oven Dry
 11 %Tangential Shrinkage Green to Oven Dry
 11 %Tangential; Green to Zero Moisture
 18.7 %Volumetric Shrinkage Green to Oven Dry
 
Descriptive Properties
ColorPink to dark redUsual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Australian Karri Wood
Fibre Glast 1069 3K, 2x2 Twill Weave Carbon Fiber Fabric
301 Stainless Steel
American Ash Wood
American Ponderosa Pine Wood

PTSO010 / 71371

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.