Data is based on small, clear, air-dried samples unless specified. Usual surface texture: Medium Dimensional changes when dried lumber is subjected to variations in humidity during service: Medium Resistance to fungal decay (Heartwood in ground contact): Very Durable (Over 25 years) Resistance to penetration by preservatives: Extremely resistant Common Applications: Heavy constructional work. Flooring |
Eucalyptus marginata; Lumber, Timber |