MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Park Aerospace Nelcote® V-341 Polybutadiene Prepreg, 503 Quartz Reinforced
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.

Key Features and Benefits:

  • Extremely low Dk/Df values for demanding RF / microwave applications
  • Self adhesive bond to foam cores
  • Long ambient out-time for easy processing
  • Easily processed in both vacuum/oven and autoclave processes
  • A cost effective, shop-friendly alternative to BMI and Cyanate Ester materials in many applications
  • Resistant to fungus, moisture, rain impact, and most chemicals

Applications/Qualifications:

  • High performance radomes
  • Signature control devices
  • US Army Helicopter
  • Air Force Ground-Based Radar

Information provided by Park Electrochemical Corp.

Key Words: PB
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 2.0 %
@Temperature 288 °C
10 min
Water Absorption 0.050 %14 days immersion
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 67
Tensile Strength, Yield 62000 psi
@Temperature 93.3 °C
0° Direction, Dry; ASTM D638
 73000 psi
@Temperature 23.9 °C
0° Direction, Dry; ASTM D638
Tensile Modulus 2900 ksi
@Temperature 23.9 °C
0° Direction, Dry; ASTM D638
Flexural Strength 25.0 ksi
@Temperature 93.3 °C
Dry; ASTM D790
 28.0 ksi
@Temperature 93.3 °C
Dry; Post-Cure; ASTM D790
 50.0 ksi
@Temperature 23.9 °C
Dry; Post-Cure; ASTM D790
 54.0 ksi
@Temperature 23.9 °C
Dry; ASTM D790
Flexural Modulus 1700 ksi
@Temperature 93.3 °C
Dry; Post-Cure; ASTM D790
 2200 ksi
@Temperature 93.3 °C
Dry; ASTM D790
 2700 ksi
@Temperature 23.9 °C
Dry; Post-Cure; ASTM D790
 2900 ksi
@Temperature 23.9 °C
Dry; ASTM D790
Compressive Strength 22.0 ksi
@Temperature 93.3 °C
Dry; Post-Cure; ASTM D695
Compressive Modulus 2900 ksi
@Temperature 93.3 °C
Dry; Post-Cure
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.09
@Frequency 1e+10 Hz
 3.12
@Frequency 3.50e+10 Hz
Dissipation Factor 0.0030
@Frequency 3.50e+10 Hz
 0.0035
@Frequency 1e+10 Hz
 
Processing PropertiesOriginal ValueComments
Gel Time 1.00 - 1.50 min
@Temperature 171 °C
Shelf Life 3.00 Month
@Temperature 4.44 °C
 6.00 Month
@Temperature -17.8 °C
 
Descriptive Properties
Fungus ResistanceRated 1 (Pass)ASTM G21-70
Prepreg Resin Content (%)26-33
Rain Impact ErosionNo detrimental effect at 15 minutes2mm droplet at 1"/hr
Resin Flow (%)6-14350°F, 100psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Appeel® 20D784 Ethylene Acrylate
Dow Appeel® LSR20D751 Lidding Sealant Resin
Fujipoly Industries Sarcon® NR-HTc Gap Filler Pad
Dow Appeel® 22D843 Ethylene Acrylate
Evonik DYNAPOL® LS 412 Polyester Resin

PPARK072 / 89344

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.