MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Rogers Corporation Poron® Shock Seal™ 4790-79-9 Handheld Urethane Foam, Handheld Grade, PET Reinforced
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Extreme Impact Protection, Ultimate Reliability

  • Specifically engineered to protect sensitive components from damage caused by impact
  • Consistent cushioning performance through repeated impacts
  • Excellent compression set resistance
  • Supporting Material - Clear Polyester Film

Information provided by Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.144 g/cc0.00521 lb/in³ASTM D3574-95 Test A
 1.395 g/cc0.05040 lb/in³supporting material; ASTM D1505
Thickness 533 - 991 microns21.0 - 39.0 milRange of Thicknesses Available
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 103 MPa15000 psiF5, supporting material; ASTM D882
Elongation at Break 150 %150 %supporting material; ASTM D882
Tensile Modulus 3.45 GPa500 ksiMD, supporting material; ASTM D882
Compressive Yield Strength 0.0138 MPa
@Strain 25 %
2.00 psi
@Strain 25 %
0.2"/min. strain rate
Coefficient of Friction, Dynamic 0.400.40A/B, supporting material; ASTM D1894
Compression Set  <= 5.0 %
@Temperature 23.0 °C
<= 5.0 %
@Temperature 73.4 °F
ASTM D1667-90 Test D
 <= 10 %
@Temperature 70.0 °C
<= 10 %
@Temperature 158 °F
ASTM D3574-95 Test D
Film Tensile Strength at Break, MD 207 MPa30000 psisupporting material; ASTM D882
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 1.2 %
@Temperature 150 °C,
Time 2340 sec
1.2 %
@Temperature 302 °F,
Time 0.650 hour
supporting material
Shrinkage, TD 0.00 %
@Temperature 150 °C,
Time 2340 sec
0.00 %
@Temperature 302 °F,
Time 0.650 hour
supporting material

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded
Overview of materials for Styrene-Butadiene Copolymer, SBC
Rogers Corporation Poron® 4701-60-30 Cellular Urethane Foam
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded

PROGA935 / 138375

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.