MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass + Mineral Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.31 - 2.96 g/cc0.0473 - 0.107 lb/in³Average value: 1.64 g/cc Grade Count:55
Filler Content 10.0 - 50.0 %10.0 - 50.0 %Average value: 28.1 % Grade Count:8
Water Absorption 0.0200 - 0.300 %0.0200 - 0.300 %Average value: 0.0774 % Grade Count:21
Moisture Absorption at Equilibrium 0.0300 - 0.200 %0.0300 - 0.200 %Average value: 0.153 % Grade Count:11
Water Absorption at Saturation 0.350 - 0.500 %0.350 - 0.500 %Average value: 0.417 % Grade Count:3
Viscosity Test 55.0 - 101 cm³/g0.550 - 1.01 dl/gAverage value: 79.0 cm³/g Grade Count:4
Linear Mold Shrinkage 0.000 - 0.0160 cm/cm0.000 - 0.0160 in/inAverage value: 0.00476 cm/cm Grade Count:49
Linear Mold Shrinkage, Transverse 0.000 - 0.0130 cm/cm0.000 - 0.0130 in/inAverage value: 0.00787 cm/cm Grade Count:13
Melt Flow 2.00 - 45.0 g/10 min2.00 - 45.0 g/10 minAverage value: 16.7 g/10 min Grade Count:13
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 43.0 - 91.043.0 - 91.0Average value: 71.8 Grade Count:10
Hardness, Rockwell R 109 - 121109 - 121Average value: 118 Grade Count:16
Tensile Strength, Ultimate 46.9 - 147 MPa6800 - 21300 psiAverage value: 97.2 MPa Grade Count:43
 30.0 - 65.0 MPa
@Temperature 60.0 - 150 °C
4350 - 9430 psi
@Temperature 140 - 302 °F
Average value: 46.3 MPa Grade Count:1
Tensile Strength, Yield 58.6 - 125 MPa8500 - 18100 psiAverage value: 89.0 MPa Grade Count:14
Elongation at Break 1.00 - 10.0 %1.00 - 10.0 %Average value: 2.72 % Grade Count:47
 2.00 - 3.00 %
@Temperature 60.0 - 150 °C
2.00 - 3.00 %
@Temperature 140 - 302 °F
Average value: 2.55 % Grade Count:1
Elongation at Yield 2.00 - 5.00 %2.00 - 5.00 %Average value: 3.00 % Grade Count:3
Modulus of Elasticity 5.24 - 13.5 GPa760 - 1960 ksiAverage value: 9.54 GPa Grade Count:26
 2.70 - 7.80 GPa
@Temperature 60.0 - 150 °C
392 - 1130 ksi
@Temperature 140 - 302 °F
Average value: 4.75 GPa Grade Count:1
Flexural Yield Strength 74.5 - 220 MPa10800 - 31900 psiAverage value: 150 MPa Grade Count:47
Flexural Modulus 2.76 - 14.7 GPa400 - 2130 ksiAverage value: 8.79 GPa Grade Count:51
Compressive Yield Strength 53.8 - 124 MPa7800 - 18000 psiAverage value: 77.7 MPa Grade Count:3
Izod Impact, Notched 0.270 - 1.07 J/cm0.506 - 2.00 ft-lb/inAverage value: 0.590 J/cm Grade Count:43
 0.85424 - 0.85424 J/cm
@Temperature -30.0 - -30.0 °C
1.6003 - 1.6003 ft-lb/in
@Temperature -22.0 - -22.0 °F
Average value: 0.854 J/cm Grade Count:1
Izod Impact, Unnotched 1.60 - 5.34 J/cm3.00 - 10.0 ft-lb/inAverage value: 4.14 J/cm Grade Count:13
Izod Impact, Notched (ISO) 3.10 - 31.0 kJ/m²1.48 - 14.8 ft-lb/in²Average value: 9.54 kJ/m² Grade Count:17
 4.50 - 8.00 kJ/m²
@Temperature -30.0 - 30.0 °C
2.14 - 3.81 ft-lb/in²
@Temperature -22.0 - 86.0 °F
Average value: 6.17 kJ/m² Grade Count:3
Izod Impact, Unnotched (ISO) 37.8 - 70.0 kJ/m²18.0 - 33.3 ft-lb/in²Average value: 49.3 kJ/m² Grade Count:3
Charpy Impact Unnotched 1.30 - 4.62 J/cm²6.19 - 22.0 ft-lb/in²Average value: 2.93 J/cm² Grade Count:13
 2.10 - 4.00 J/cm²
@Temperature -30.0 - -30.0 °C
9.99 - 19.0 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 2.86 J/cm² Grade Count:9
Charpy Impact, Notched 0.400 - 1.21 J/cm²1.90 - 5.76 ft-lb/in²Average value: 0.610 J/cm² Grade Count:20
 0.400 - 0.720 J/cm²
@Temperature -30.0 - -20.0 °C
1.90 - 3.43 ft-lb/in²
@Temperature -22.0 - -4.00 °F
Average value: 0.575 J/cm² Grade Count:10
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+13 - 1.00e+17 ohm-cm1.00e+13 - 1.00e+17 ohm-cmAverage value: 1.20e+16 ohm-cm Grade Count:28
Surface Resistance 1.00e+13 - 1.00e+17 ohm1.00e+13 - 1.00e+17 ohmAverage value: 2.38e+16 ohm Grade Count:11
Dielectric Constant 3.00 - 5.103.00 - 5.10Average value: 3.80 Grade Count:16
Dielectric Strength 17.0 - 100 kV/mm432 - 2540 kV/inAverage value: 25.2 kV/mm Grade Count:25
Dissipation Factor 0.00100 - 0.04000.00100 - 0.0400Average value: 0.0149 Grade Count:16
Arc Resistance 80.0 - 130 sec80.0 - 130 secAverage value: 121 sec Grade Count:10
Comparative Tracking Index 125 - 600 V125 - 600 VAverage value: 319 V Grade Count:14
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 - 55.8 µm/m-°C10.0 - 31.0 µin/in-°FAverage value: 27.4 µm/m-°C Grade Count:18
CTE, linear, Transverse to Flow 46.0 - 97.0 µm/m-°C25.6 - 53.9 µin/in-°FAverage value: 74.1 µm/m-°C Grade Count:10
Melting Point 210 - 268 °C410 - 514 °FAverage value: 224 °C Grade Count:23
Maximum Service Temperature, Air 75.0 - 200 °C167 - 392 °FAverage value: 132 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 184 - 223 °C363 - 433 °FAverage value: 214 °C Grade Count:40
Deflection Temperature at 1.8 MPa (264 psi) 65.6 - 220 °C150 - 428 °FAverage value: 193 °C Grade Count:53
Vicat Softening Point 150 - 220 °C302 - 428 °FAverage value: 201 °C Grade Count:7
Glass Transition Temp, Tg 54.0 - 60.0 °C129 - 140 °FAverage value: 57.0 °C Grade Count:6
Flammability, UL94 HB - V-0HB - V-0Grade Count:37
Oxygen Index 20.0 - 35.0 %20.0 - 35.0 %Average value: 26.8 % Grade Count:4
Glow Wire Test 650 - 960 °C1200 - 1760 °FAverage value: 873 °C Grade Count:4
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 280 °C68.0 - 536 °FAverage value: 155 °C Grade Count:17
Nozzle Temperature 243 - 280 °C470 - 536 °FAverage value: 264 °C Grade Count:5
Die Temperature 240 - 265 °C464 - 509 °FAverage value: 252 °C Grade Count:9
Melt Temperature 225 - 280 °C437 - 536 °FAverage value: 250 °C Grade Count:28
Mold Temperature 26.7 - 120 °C80.0 - 248 °FAverage value: 81.6 °C Grade Count:27
Injection Velocity 300 mm/sec11.8 in/secAverage value: 300 mm/sec Grade Count:9
Drying Temperature 104 - 140 °C220 - 284 °FAverage value: 122 °C Grade Count:19
Moisture Content 0.0200 - 0.0300 %0.0200 - 0.0300 %Average value: 0.0208 % Grade Count:12
Injection Pressure 48.0 - 140 MPa6960 - 20300 psiAverage value: 76.2 MPa Grade Count:12
Hot-Working Temperature 250 - 265 °C482 - 509 °FAverage value: 257 °C Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polybutylene Terephthalate (PBT), Aramid Fiber Filled
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled

O3238 / 78182

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.