MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Medalist® MD-34060 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Medalist MD-34060 is a high performance thermoplastic elastomer specifically designed for overmolding and multi-shot molding applications in the healthcare/medical segment. Medalist MD-34060 is a medium hardness, medium density, halogen-free grade that bonds to ABS, PC/ABS, and PC.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Abrasion Resistant; Bondability; Chemical Resistant; Ethylene Oxide Sterilizable; Filled, Good Colorability; Good Flexibility; Good Flow; Good Impact Resistance; Good Moldability; Good Scratch Resistance; Good Sterilizability; Halogen Free; Lubricated; Medium Density; Medium Hardness; Radiation Sterilizable; Steam Sterilizable

Uses: Bonding; Medical/Healthcare Applications; Overmolding; Soft Touch Applications

Agency Ratings: ISO 10993 Part 5; ISO 13485

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Multi Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ASTM D792
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  60
@Time 5.00 sec
60
@Time 0.00139 hour
Injection Molded; ASTM D2240
 61
@Time 1.00 sec
61
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 8.83 MPa1280 psiDie C, 20 in/min; ASTM D412
Tensile Stress at Strain  2.00 MPa
@Strain 100 %
290 psi
@Strain 100 %
Die C, 20 in/min; ASTM D412
 3.65 MPa
@Strain 300 %
530 psi
@Strain 300 %
Die C, 20 in/min; ASTM D412
Elongation at Break 650 %650 %Die C, 20 in/min; ASTM D412
Tear Strength 41.2 kN/m235 pliASTM D624
Peel Strength 2.63 kN/m15.0 pliAdhesion to PC
 2.80 kN/m16.0 pliAdhesion to ABS
 4.21 kN/m24.0 pliAdhesion to PC/ABS
Compression Set 37 %
@Temperature 22.8 °C,
Time 79200 sec
37 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395B
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 160 - 182 °C320 - 360 °F
Middle Barrel Temperature 193 - 221 °C380 - 430 °F
Front Barrel Temperature 182 - 199 °C360 - 390 °F
Nozzle Temperature 182 - 199 °C360 - 390 °F
Melt Temperature 182 - 204 °C360 - 400 °F
Mold Temperature 15.6 - 32.2 °C60.0 - 90.0 °F
Back Pressure 0.172 - 0.689 MPa25.0 - 100 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceColors Available
 Natural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Medalist® MD-32265 Thermoplastic Elastomer
Teknor Apex Medalist® MD-34065 Thermoplastic Elastomer
Teknor Apex Medalist® MD-12362 Thermoplastic Elastomer
Teknor Apex Medalist® MD-12160H Thermoplastic Elastomer
Covestro Apec® 1745 Polycarbonate

PTEKNQ0722 / 237213

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.